Aspectus et conditio: album (perlucidum vel translucidum) obstupefactum
Monomeri tertii generis et content: ENB, 9%
Ethylene content: 60%
Mooney viscositas: ML (1+4) 125°C 92
Magnitudo: 25kg/obstructionum
MOQ: 25kg
sarcina: cohibenti
Aspectus et conditio: album (perlucidum vel translucidum) obsitum
Tertium monomerorum genus et contentum: ENB, 8.5%
Ethylene contentum: 60%
Mooney viscositas: ML (1+4) 125°C 84 ML (1+4) 150℃ 81
Magnitudo: 25kg/obstructionum
MOQ: 25kg
sarcina: cohibenti
Aspectus et conditio: album (perlucidum vel translucidum) obstupefactum
tertium genus monomerorum et contentum: ENB, 5.7%
contentum Ethylene: 70%
contentum olei: 50%
viscositas Mooney: ML (1+4) 125°C 53
Magnitudo: 25kg/ scandalum
MOQ: 25kg
sarcina: cohibenti
Aspectus et conditio: album (perlucidum vel translucidum) obsitum
TERTIUM monomerorum genus et contentum: ENB, 1.9%
Ethylene content: 57.8%
viscositas Mooney: ML (1+4) 125°C 44
Magnitudo: 25kg/obstructionum
MOQ: 25kg
sarcina: cohibenti
Aspectus et conditio: album (perlucidum vel translucidum) obstupefactum
tertium genus monomerorum et contentum: ENB, 2.0%
Ethylene content: 62%
viscositas Mooney: ML (1+4) 125°C 53
Magnitudo: 25kg/obstructionum
MOQ: 25kg
sarcina: cohibenti
Color: Colorful(customizable)
appearance:Blocks or stripes (customizable)
Vulcanization type:peroxide
Mooney viscositas ML (1+4) 100℃:45-55
Hardness:60±5 Litus
tensile strength:min.10 Mpa
Elongatio ad break:min.300%
MOQ: 150kg
Expiration date: Tres menses