swa dutral na vaphakeri eChina lava nga kotaka ku xavisa hi wholesale
dutral . Hi nga ku nyika vukorhokeri bya xiphurofexinali na nxavo wo antswa eka wena. Loko u tsakela switirhisiwa swa
DUTRAL , hi kombela u tihlanganisa na hina. Switsundzuxo: Swilaveko swo hlawuleka, xikombiso: OEM, ODM, leyi endleriweke hi ku ya hi swilaveko, dizayini na swin’wana, hi kombela u hi rhumela imeyili na ku hi byela swilaveko swa vuxokoxoko. Hi landzelela khwalithi ya ku wisa hi tiyisisa leswaku nxavo wa ripfalo, vukorhokeri lebyi tinyiketeleke.
Ku languteka na xiyimo: Beige kumbe pale yellow blocky
Muxaka wa vunharhu wa monomer na nhlayo: ENB, 4.5%
Ethylene: 55.5%
Mooney viscosity: ML(1+4)125°C 55
Vukulu: 25kg/block
MOQ: 25kg
Ku paka: boxed
Ku languteka na xiyimo: Beige kumbe pale yellow blocky
third monomer muxaka na nhundzu: ENB, 8.5%
ethylene content: 52.5%
Mooney viscosity: ML(1+4)125°C 68
mafurha ya le ndzeni: 20%
Vukulu: 25kg/block
MOQ: 25kg
Packing:
Ku languteka na xiyimo: Beige kumbe pale yellow blocky
Muxaka wa vunharhu wa monomer na nhlayo: ENB, 7%
Ethylene: 53%
Mooney viscosity: ML(1+4)125°C 65
Nhlayo ya oyili: 18%
Vukulu: 25kg/block
MOQ: 25kg
Ku paka: ebokisini
Ku languteka na xiyimo: Beige kumbe muhlovo wo tshwuka wo tshwuka wa blocky
muxaka wa monomer wa vunharhu na nhundzu: ENB, 4%
Ethylene Nhlayo ya le henhla: 61%
Mooney Viscosity: ML(1+4)100°C 44
Vukulu: 25kg/block
MOQ: 25kg
Ku paka: Bokisi
Ku languteka na xiyimo: Beige kumbe pale yellow blocky
third monomer muxaka na nhundzu: ENB, 4.5%
Ethylene content: 59.5%
Mooney viscosity: ML(1+4)125°C 47
Mafurha ya le ndzeni:10%
Vukulu: 25kg/block
Moq: 25kg
Packing:
Ku languteka na xiyimo: Beige kumbe pale yellow blocky
Muxaka wa vunharhu wa monomer na nhlayo: ENB, 4.5%
Ethylene: 63.5%
Mooney viscosity: ML(1+4)125°C 57
Nhlayo ya oyili: 67%
Vukulu: 25kg/block
MOQ: 25kg
Ku paka: boxed