Herchy i vaendli va swilo
swa dutral na vaphakeri eChina lava nga kotaka ku xavisa hi wholesale
dutral . Hi nga ku nyika vukorhokeri bya xiphurofexinali na nxavo wo antswa eka wena. Loko u tsakela switirhisiwa swa
DUTRAL , hi kombela u tihlanganisa na hina. Switsundzuxo: Swilaveko swo hlawuleka, xikombiso: OEM, ODM, leyi endleriweke hi ku ya hi swilaveko, dizayini na swin’wana, hi kombela u hi rhumela imeyili na ku hi byela swilaveko swa vuxokoxoko. Hi landzelela khwalithi ya ku wisa hi tiyisisa leswaku nxavo wa ripfalo, vukorhokeri lebyi tinyiketeleke.
Ku languteka na xiyimo: Beige kumbe pale yellow blocky
third monomer muxaka na nhundzu: ENB, 4.5%
Ethylene content: 59.5%
Mooney viscosity: ML(1+4)125°C 47
Mafurha ya le ndzeni:10%
Vukulu: 25kg/block
Moq: 25kg
Packing:
Ku languteka na xiyimo: Beige kumbe pale yellow blocky
Muxaka wa vunharhu wa monomer na nhlayo: ENB, 5.5%
Ethylene: 66.5%
Mooney viscosity: ML(1+4)125°C 43
Nhlayo ya oyili: 67%
Vukulu: 25kg/block
MOQ: 25kg
Ku paka: boxed
Ku languteka na xiyimo: Beige kumbe pale yellow blocky
Muxaka wa vunharhu wa monomer na nhlayo: ENB, 4.4%
Ethylene: 68.6%
Mooney viscosity: ML(1+4)125°C 60
Vukulu: 25kg/block
MOQ: 25kg
Ku paka: boxed
Ku languteka na xiyimo: Beige kumbe pale yellow blocky
Muxaka wa vunharhu wa monomer na nhlayo: ENB, 8.9%
Ethylene: 60.1%
Mooney viscosity: ML(1+4)100°C 64
Vukulu: 25kg/block
MOQ: 25kg
Ku paka: boxed