ʻO Herchy ma ke ʻano he mea hana ʻoihana a me ka mea hoʻolako ma Kina, ua hala nā
Dutral āpau
Dutral i nā kūlana hōʻoia ʻoihana honua, a hiki iā ʻoe ke hōʻoiaʻiʻo i ka maikaʻi. Inā ʻaʻole ʻoe e ʻike i kāu Intent
Dutral i kā mākou papa inoa huahana, hiki iā ʻoe ke hoʻokaʻaʻike mai iā mākou, hiki iā mākou ke hāʻawi i nā lawelawe maʻamau.
ʻO ka hiʻohiʻona a me ke kūlana: Beige a pale melemele ʻeleʻele
ʻO ke ʻano monomer ʻekolu a me ka maʻiʻo: ENB, 7,4%
Ethylene maʻiʻo: 60,6%
Mooney viscosity: ML (1 + 4) 125 ° C 33
ʻO ka ʻaila maʻiʻo: 30%
Nui: 25kg / poloka
MOQ: 25kg
Hoʻopili: pahu
ʻO ke ʻano a me ke kūlana: Beige a ʻeleʻele ʻeleʻele blocky
ʻO ke ʻano monomer ʻekolu a me ka maʻiʻo: ENB, 8.5%
Ethylene maʻiʻo: 52.5%
Mooney viscosity: ML (1 + 4) 125 ° C 68
ʻAiʻa maʻiʻo: 20%
Nui: 25kg / poloka
MOQ: 25kg
Hoʻopili: pahu
ʻO ka hiʻohiʻona a me ke kūlana: Beige a ʻeleʻele ʻeleʻele blocky
ʻO ke ʻano monomer ʻekolu a me ka ʻike: ENB, 7%
Ethylene maʻiʻo: 53%
Mooney viscosity: ML (1 + 4) 125 ° C 65
ʻO ka ʻaila maʻiʻo: 18%
Nui: 25kg / poloka
MOQ: 25kg
Hoʻopili: pahu
ʻO ka hiʻohiʻona a me ke kūlana: Beige a ʻeleʻele ʻeleʻele blocky
ʻO ke ʻano monomer ʻekolu a me ka ʻike: ENB, 4%
Ethylene maʻiʻo: 61%
Mooney viscosity: ML (1 + 4) 100 ° C 44
Nui: 25kg / poloka
MOQ: 25kg
Pākuʻi: pahu
ʻO ke ʻano a me ke kūlana: Beige a i ʻole ʻeleʻele melemele blocky
ʻO ke ʻano monomer ʻekolu a me ka maʻiʻo: ENB, 4.5%
Ethylene maʻiʻo: 59.5%
Mooney viscosity: ML (1 + 4) 125 ° C 47
ʻO ka ʻaila maʻiʻo: 10%
Nui: 25kg / poloka
MOQ: 25kg
Hoʻopili: pahu pahu
ʻO ka hiʻohiʻona a me ke kūlana: Beige a ʻeleʻele ʻeleʻele blocky
ʻO ke ʻano monomer ʻekolu a me ka maʻiʻo: ENB, 4.5%
Ethylene maʻiʻo: 63.5%
Mooney viscosity: ML (1 + 4) 125 ° C 57
ʻAiʻa maʻiʻo: 67%
Nui: 25kg / poloka
MOQ: 25kg
Hoʻopili: pahu