Herchy is Dutral manufacturers and suppliers in China who can wholesale Dutral. We can provide professional service and better price for you. If you interested in Dutral products, please contact with us. Tips: Special needs, for example: OEM, ODM, customized according to demands, design and others, please email us and tell us detail needs. We follow the quality of rest assured that the price of conscience, dedicated service.
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 4.5% Ethylene content: 55.5% Mooney viscosity: ML(1+4)125°C 55 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 8.5% Ethylene content: 52.5% Mooney viscosity: ML(1+4)125°C 68 Oil content:20% Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 4% Ethylene content: 61% Mooney viscosity: ML(1+4)100°C 44 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: Beige or pale yellow blocky Third monomer type and content: ENB, 4.4% Ethylene content: 68.6% Mooney viscosity: ML(1+4)125°C 77 Size: 25kg/block MOQ: 25kg Packing: boxed