Ponahalo le boemo: Beige kapa mosehla o mosehla blocky
Mofuta oa boraro oa monomer le litaba: ENB, 4.5%
Likahare tsa ethylene: 55.5%
Mooney viscosity: ML (1+4) 125 ° C 76
Boholo: 25kg / thibela
MOQ: 25kg
Ho paka: lebokose
Ponahalo le boemo: Beige kapa mosehla o mosehla blocky
Mofuta oa boraro oa monomer le litaba: ENB, 4.4%
Likahare tsa ethylene: 68.6%
Mooney viscosity: ML (1+4) 125 ° C 60
Boholo: 25kg / thibela
MOQ: 25kg
Ho paka: lebokose