ʻO ka hiʻohiʻona a me ke kūlana: Beige a pale melemele ʻeleʻele
ʻO ke ʻano monomer ʻekolu a me ka maʻiʻo: ENB, 7,4%
Ethylene maʻiʻo: 60,6%
Mooney viscosity: ML (1 + 4) 125 ° C 33
ʻO ka ʻaila maʻiʻo: 30%
Nui: 25kg / poloka
MOQ: 25kg
Hoʻopili: pahu
ʻO ka hiʻohiʻona a me ke kūlana: Beige a ʻeleʻele ʻeleʻele blocky
ʻO ke ʻano monomer ʻekolu a me ka ʻike: ENB, 4.5%
Ethylene maʻiʻo: 55.5%
Mooney viscosity: ML (1 + 4) 125 ° C 76
Nui: 25kg / poloka
MOQ: 25kg
Hoʻopili: pahu pahu
ʻO ka hiʻohiʻona a me ke kūlana: Beige a pale melemele ʻeleʻele
ʻO ke ʻano monomer ʻekolu a me ka maʻiʻo: ENB, 4.4%
Ethylene maʻiʻo: 68.6%
Mooney viscosity: ML (1 + 4) 125 ° C 60
Nui: 25kg / poloka
MOQ: 25kg
Hoʻopili: pahu pahu
ʻO ke ʻano a me ke kūlana: Beige a ʻeleʻele ʻeleʻele blocky
ʻO ke ʻano monomer ʻekolu a me ka maʻiʻo: ENB, 5.5%
Ethylene maʻiʻo: 66.5%
Mooney viscosity: ML (1 + 4) 125 ° C 43
ʻO ka ʻaila maʻiʻo: 67%
Nui: 25kg / poloka
MOQ: 25kg
Hoʻopili: pahu
ʻO ka hiʻohiʻona a me ke kūlana: Beige a ʻeleʻele ʻeleʻele blocky
ʻO ke ʻano monomer ʻekolu a me ka ʻike: ENB, 8%
Ethylene maʻiʻo: 60%
Mooney viscosity: ML (1 + 4) 125 ° C 43
ʻO ka ʻaila ʻaila: 100%
Nui: 25kg / poloka
MOQ: 25kg
Hoʻopili: pahu pahu