GA-99X1 Low Compression Set Silicone Rubber (HCR)
Kushanda: kwakakodzera kugadzirwa kwemhete yekuisa chisimbiso, machira, auto zvikamu uye zvimwe zvigadzirwa.
Chinhu chakakosha: kusimba kwepamusoro, kudzika kwakadzika kweseti, isina-chepfu isina kuravira HSE, pfuura kusimbiswa kweRoHS, REACH uye FDA.