Ubucucike Buke bwa Ethylene Propylene Diene Monomer-EPDM
Ibara: Umukara (guhindurwa)
kugaragara cks Guhagarika cyangwa imirongo (byemewe)
Ubwoko bwa Vulcanisation : peroxide
Mooney viscosity ML (1 + 4) 100 ℃: 65-75
Gukomera : 60 ± 5 Inkombe Imbaraga
zingana : min.10 Mpa
Kurambura kuruhuka : min.300%
MOQ: 150kg
Itariki yo kurangiriraho: amezi atatu