Hiri Hiiri iti Ethylene Propylene Diene Monomer-EPDM
Tae: Pango(ka taea te whakarite)
te ahua: Poraka, takai ranei (ka taea te whakarite)
Momo whakangao: peroxide
Mooney viscosity ML(1+4)100℃:65-75
Te pakeke:60±5 Shore A
Te kaha Tensile:min.10 Mpa
Elongation i te wehenga:min.300%
MOQ: 1500% MOQ: 1500
% MOQ