I-Low Density Seals Ethylene Propylene Diene Monomer-EPDM
Umbala: Mnyama (okungenzeka ngokwezifiso)
ukubukeka:Amabhulokhi noma amapheshana (okungezifiso)
Uhlobo lwe-vulcanization:i-peroxide
Mooney viscosity ML(1+4)100℃:65-75
Ukuqina:60±5 Shore A
Amandla Aqinile:min.10 Mpa
Ubude ngesikhathi sekhefu:min.300 idethi ye-
1kg:
Izinyanga ezintathu ze -MOQ: