synthetic rubbers: eby’obugagga ebikwata ku nsonga, ebirungi, n’okukozesebwa .

1. Fluororubber (FKM) .

  • Eby'bwanannyini:

    • Okuziyiza ebbugumu erisukkiridde (-20°C okutuuka ku +250°C).

    • Okuziyiza okw’enjawulo eri amafuta, amafuta, ebiziyiza, asidi, ne base.

    • Amaanyi g’okusika amangi, compression set entono, n’okutebenkera kw’eddagala okulungi ennyo.

    • Egumira ennimi z’omuliro ate nga tegumira ozone.

  • Ebirungi:

    • Agumira eddagala ery’amaanyi n’embeera za puleesa enkulu.

    • Obulamu obuwanvu mu kukola emirimu mu by’ennyonyi n’emmotoka.

  • Okusaba:

    • Enkola y’amafuta mu nkola y’amafuta, O-rings, ne gaasikiti.

    • Automotive transmission seals, hose za yingini, n’ebitundu bya turbocharger.

    • Ebikozesebwa mu kulongoosa eddagala linings ne gaskets.

2. Omupiira gwa Chloroprene (CR) .

  • Eby'bwanannyini:

    • Okuziyiza amafuta ag’ekigero (okusinga gapiira ag’obutonde naye nga matono okusinga FKM).

    • Flame retardant nga erina eby’obugagga eby’okwezimbulukuka.

    • Obuziyiza bw’obudde bulungi (UV, ozone, n’obunnyogovu).

    • Ekyukakyuka ku bbugumu eri wansi (-40°C okutuuka ku +120°C).

  • Ebirungi:

    • Ekendeeza ku nsimbi nga nnyangu okukola (extrusion/molding).

    • amaanyi amangi ag’ebyuma n’okuziyiza okusika.

  • Okusaba:

    • Essuuti ezirimu amazzi, ggalavu, ne hoosi z’amakolero.

    • adhesives z’engatto n’okuzimba.

    • obukooti bwa cable n’obuwuka obuzimba akasolya.

3. Omupiira gwa Nitrile ogulina haidrojeni (HNBR) .

  • Eby'bwanannyini:

    • Okuziyiza ebbugumu okunywezeddwa (okutuuka ku +150°C) bw’ogeraageranya ne NBR.

    • Obuziyiza obw’ekika ekya waggulu eri amafuta, amazzi g’amazzi, ne amine.

    • amaanyi amangi ag’okusika n’okuziyiza obukoowu.

    • Okuyita okutono eri ggaasi.

  • Ebirungi:

    • Akuuma obugumu (elasticity) wansi w’okumala ebbanga eddene ng’akwatibwa eddagala erikambwe.

    • Obulamu obuwanvu okusinga NBR mu mbeera ezisukkiridde.

  • Okusaba:

    • Ebikozesebwa mu kusima amafuta ne ggaasi (abapakinga, ebisiba).

    • Emisipi gy’okuteeka amafuta mu mmotoka, ebitundu ebifuyira amafuta, n’ebisiba ebikuba ebyuma ebiyitibwa turbocharger seals.

    • Siliinda z’amazzi ez’amakolero.

4. Omupiira gwa silikoni (VMQ) .

  • Eby'bwanannyini:

    • Ebbugumu erya ultra-wide (-60°C okutuuka ku +200°C).

    • Elasticity enkulu (okutuuka ku 1000% elongation).

    • Okuziyiza amasannyalaze okulungi ennyo n’okunyweza ebbugumu.

    • Biocompatible ate nga tekola.

  • Ebirungi:

    • Ekuuma obugonvu mu mbeera ezikola cryogenic ne high-temperature.

    • Egumikiriza UV, ozone, n’obudde.

  • Okusaba:

    • ebyuma eby’obujjanjabi (catheters, implants).

    • Ebitundu by’ebyuma (ebiziyiza, ebisumuluzo).

    • Gaasi ezirimu ebbugumu eringi eri oven ne yingini.

5. Omupiira gwa Fluorosilicone (FVMQ) .

  • Eby'bwanannyini:

    • Egatta obuziyiza bwa FKM obw’eddagala n’obugonvu bwa VMQ.

    • Ebbugumu eriri wakati wa: -50°C okutuuka ku +230°C.

    • Egumira amafuta, ebizigo, n’amazzi agakulukuta.

    • Low compression set n’okugumira obulungi.

  • Ebirungi:

    • Akola mu bitundu byombi eby’ebbugumu eringi n’eby’ebbugumu eri wansi.

    • Okuziyiza okuzimba mu mafuta g’ennyonyi.

  • Okusaba:

    • Ebitundu by’enkola y’amafuta g’ennyonyi (valves, seals).

    • Gaasi n’ebiyungo ebinywera mu nnyanja ennene.

    • sensa z’emmotoka n’enkola ezifuga omukka ogufuluma mu mmotoka.

6. ethylene propylene diene monomer (EPDM) .

  • Eby'bwanannyini:

    • Ozone ow'enjawulo n'okuziyiza embeera y'obudde.

    • Amaanyi ga dielectric aga waggulu n’okuziyiza amazzi.

    • Ebbugumu eriri wakati wa: -50°C okutuuka ku +150°C.

    • Okuyita kwa ggaasi okutono.

  • Ebirungi:

    • Ebisinga okukendeeza ku ssente mu kukozesebwa ebweru.

    • Excellent vibration damping n'okukendeeza ku maloboozi.

  • Okusaba:

    • Automotive WeatherStripping, radiator hoses, ne windshield seals.

    • Ebiwujjo by’okuzimba akasolya n’ebidiba.

    • Okuziyiza waya z’amasannyalaze n’emisipi egy’okutambuza amaanyi.


ENKOZESA Y'AMAWANGA

EBINTU EBYAFFE

AMAWULIRE AG'OKUKWATAGANA

Okwongerako: No.33, Lane 159, oluguudo lwa Taiye, mu Disitulikiti y’e Fengxian, Shanghai
Essimu / WhatsApp / Skype: +86 15221953351 ku ssimu
Eddembe ly’okuwandiika     2023 Kkampuni ya Shanghai Herchy Rubber Co., Ltd. Sitemap y'ekifo |   Enkola y'Ebyama | Obuwagizi bwa . Leadong.