Sintetik rɔba dɛn: Ditayla prɔpati dɛn, advantej dɛn, ɛn aplikeshɔn dɛn

1. Fluororubber (FKM)

  • Prɔpati dɛn:

    • Ekstrim tempɔret rɛsistɛns (-20°C to +250°C).

    • Eksepshɔnal resistans to ɔyl, fiul, sɔlvɛnt, asid, ɛn bays.

    • Ay tɛnsiɛl trɛnk, lɔw kɔmpreshɔn sɛt, ɛn fayn fayn kemikal stebiliti.

    • Flame-resistant ɛn ozon-resistant.

  • Di bɛnifit dɛn we pɔsin kin gɛt:

    • Witstand agresiv kemikal ɛn ay-prɛshɔn ɛnvayrɔmɛnt.

    • Long savis layf in aerospace ɛn ɔtomotiv aplikeshɔn dɛn.

  • Aplikeshɔn dɛn:

    • Aircraft fuel system sil, O-ring, ɛn gasket.

    • Otomotiv transmishɔn sil, injin hos, ɛn turbocharger kɔmpɔnɛnt dɛn.

    • Kεmikכl prכsεsin ikwipmεnt layn dεm εn gaskεt dεm.

2. Klɔroprɛn rɔba (CR) .

  • Prɔpati dɛn:

    • Modaret ɔyl rɛsistɛns (bɛtɛ pas natura rɔba bɔt smɔl pas FKM).

    • Flame retardant wit self-extinguishing prɔpati.

    • Gud wɛda rɛsistɛns (UV, ɔzoyn, ɛn mɔstɔ).

    • Fleksibul na lɔw tɛmpracha (-40°C to +120°C).

  • Di bɛnifit dɛn we pɔsin kin gɛt:

    • Kɔst-ɛfɛktiv wit izi prɔsesin (ɛkstrushɔn/mɔlding).

    • Ay mɛkanikal trɛnk ɛn abrashɔn rɛsistɛns.

  • Aplikeshɔn dɛn:

    • Wet suit, glɔv, ɛn industrial hos.

    • Adhesives fɔ sus ɛn kɔnstrɔkshɔn.

    • Kebul jakit ɛn ruf mɛmbran dɛn.

3. Haydrojen naytrayl rɔba (HNBR) .

  • Prɔpati dɛn:

    • Enhansed heat resistans (up to +150°C) kompare to NBR.

    • supia resistans to oil, haydrolik fluid, ɛn amin.

    • ay tɛnsiɛl trɛnk ɛn taya rɛsistɛns.

    • Low permeabiliti fɔ gas dɛn.

  • Di bɛnifit dɛn we pɔsin kin gɛt:

    • i de kip elastisiti ɔnda prolɔng ɛksplɔshɔn to harsh kemikal dɛn.

    • Lכng layfspan pas NBR in ekstrim kondishכn.

  • Aplikeshɔn dɛn:

    • Ɔyl ɛn gas drɔlin tul dɛn (pak, sil).

    • Ɔtomotiv Taymin Bɛlt, Fiul Injɛkshɔn Kɔmpɔnɛnt dɛn, ɛn Turbocharger Sil dɛn.

    • Indastrial Haydrolik silinda dɛn.

4. silikon raba (VMQ) .

  • Prɔpati dɛn:

    • Ultra-wayd tempɔret rɛnj (-60°C to +200°C).

    • ay elastisiti (we go rich 1000% elongeshɔn).

    • Ekselen ilektrikal insuleshɔn ɛn tɛmral stebiliti.

    • Bayokɔmpatibl ɛn inɛt.

  • Di bɛnifit dɛn we pɔsin kin gɛt:

    • Mentɛn fleksibiliti insay krayojɛnik ɛn ay-tɛmpracha ɛnvayrɔmɛnt.

    • I nɔ de fɛt UV, Ozon, ɛn i de wet.

  • Aplikeshɔn dɛn:

    • Medikal Divays (Cateters, Implants).

    • Ilɛktronik kɔmpɔnɛnt dɛn (insulɛta dɛn, kipad dɛn).

    • Gasket dɛn we gɛt ay tempɔret fɔ ɔvin ɛn injin dɛn.

5. Fluorosilicone rubber (FVMQ) .

  • Prɔpati dɛn:

    • Kɔmbayn FKM in kemikal rɛsistɛns ɛn VMQ in fleksibiliti.

    • Tempracha renj: -50°C to +230°C.

    • I nɔ de taya fɔ yuz fiul, lɔbrik, ɛn haydrolik wata.

    • Low compression set ɛn gud resiliɛns.

  • Di bɛnifit dɛn we pɔsin kin gɛt:

    • Pɔfɔm in ɔl tu di ay-tɛmpracha ɛn lɔw-tɛmpracha ekstrim.

    • Resistant to swelling in avieshɔn fiul dɛn.

  • Aplikeshɔn dɛn:

    • Di komponent dɛn we de na di plen in fiul sistem (valv, sil).

    • Dip-si sɔbmarsibl gasket ɛn kɔnɛkta dɛn.

    • Otomotiv sensor ɛn emishɔn kɔntrol sistem.

6. Ethylene Propylene Diene Monomer (EPDM) .

  • Prɔpati dɛn:

    • Ɔdasayz ɔzoyn ɛn wɛda rɛsistɛns.

    • ay dayelɛktrik trɛnk ɛn wata rɛsistɛns.

    • Tempracha renj: -50°C to +150°C.

    • Low gas permeabiliti.

  • Di bɛnifit dɛn we pɔsin kin gɛt:

    • Mɔs pan di kɔst-ɛfɛktiv fɔ ɔda aplikeshɔn dɛn na do.

    • Eksɛlɛnt vaybreshɔn damp ɛn nɔys ridɔkshɔn.

  • Aplikeshɔn dɛn:

    • Awtmotiv Wetastripin, Radiator hos, ɛn winda sil dɛn.

    • Ruf mɛmbran ɛn pɔnd layn dɛn.

    • Ilektrikal kebul insuleshɔn ɛn pawa transmishɔn bɛlt dɛn.


KWƐK LINK DƐN

WI PRODƆKT DƐN

INFƆMƐSHƆN FƆ KƆNTƐKT

Add: No.33, Lane 159, Taiye Rod, Fengxian Distrikt, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Kopirayt     2023 Shanghai Herchy Rɔba Kɔmni, Ltd. Saytmap . |   Prayvesi Polisi | Sɔpɔt bay . Leadong.