Tel: +86 15221953351 E-mail: | ' }else if(value == "1" || value == "4" || value == "7" || value == "14"){ var langDivMid = ' ' }else if(value == "2" || value == "12" || value == "5" || value == "8"){ var langDivMid = ' / ' }else{ var langDivMid = ' | ' } if(newArr.length >= 0){ el.find("span").remove(); for (var i = 0; i < newArr.length; i++) { el.append(newArr[i]) if(i == newArr.length-1){ }else{ el.append(langDivMid) } } } }else{ //下拉风格 for (var i = 0; i < data.length; i++) { el.find(".lang-item").each(function () { if (data[i].isDefault == "0") { if ($(this).attr("data-default") == "0") { if ($(this).attr("data-lancode") == data[i].islanCode) { var cloneSpan = $(this).clone(true) newArr.push(cloneSpan) } } } else { if ($(this).attr("data-default") == "1") { if ($(this).attr("data-lancode") == data[i].islanCode) { //newArr.push($(this)) var cloneSpan = $(this).clone(true) newArr.push(cloneSpan) } } } }) } if(newArr.length >= 0){ el.find(".lang-item").remove(); for (var i = 0; i < newArr.length; i++) { if(value == "13"){ el.find(".langBar-easystyle-sub").append(newArr[i]) }else{ el.find(".lang-menu").append(newArr[i]) } } } } } // 组件包裹框注册 $(function(){ var dom = $(".sitewidget-langBar-20230302122131 .sitewidget-bd .lang-bar"); var sortArr = [{"id":0,"islanCode":"5","isDefault":"0"},{"id":1,"islanCode":"0","isDefault":"0"},{"id":2,"islanCode":"3","isDefault":"0"},{"id":3,"islanCode":"16","isDefault":"0"},{"id":4,"islanCode":"29","isDefault":"0"},{"id":5,"islanCode":"30","isDefault":"0"}]; if(sortArr != "" && sortArr != undefined){ sortableli(dom,sortArr,15) } var iconEl = $(".sitewidget-langBar-20230302122131 .lang-bar .front-icon-box") if(iconEl.length > 0){ $(".sitewidget-langBar-20230302122131 .lang-bar .lang-dropdown .lang-selected").prepend(iconEl) } }); }catch(e){try{console && console.log && console.log(e);}catch(e){}}
  • Rubbers sịntetik: Njirimara zuru oke, uru na ngwa

    1. Fluororubber (FKM)

    • Njirimara:

      • Nnukwu nguzogide okpomọkụ (-20°C ruo +250°C).

      • Nguzogide pụrụiche megide mmanụ, mmanụ ọkụ, ihe mgbaze, acids na ntọala.

      • Ike tensile dị elu, ntọala mkpakọ dị ala, yana nkwụsi ike kemịkalụ mara mma.

      • Ọkụ na-eguzogide ọkụ na ozone na-eguzogide.

    • Uru:

      • Na-eguzogide kemịkalụ ike na gburugburu oke nrụgide.

      • Ogologo ndụ ọrụ na ikuku ikuku na ngwa ụgbọ ala.

    • Ngwa:

      • Usoro mmanụ ụgbọ elu, O-mgbanaka, na gaskets.

      • Akara nnyefe akpaaka, hoses engine, na akụrụngwa turbocharger.

      • Kemịkalụ nhazi akụrụngwa lining na gaskets.

    2. Chloroprene roba (CR)

    • Njirimara:

      • Nguzogide mmanụ na-agafeghị oke (dị mma karịa rọba eke mana ọ na-erughị FKM).

      • Ọkụ na-egbochi ọkụ nwere ihe na-emenyụ onwe ya.

      • Ezigbo nguzogide ihu igwe (UV, ozone, na mmiri).

      • Na-agbanwe agbanwe na obere okpomọkụ (-40°C ruo +120°C).

    • Uru:

      • Ọnụ-irè na mfe nhazi (extrusion / ịkpụzi).

      • Ike igwe dị elu na mgbochi abrasion.

    • Ngwa:

      • Suut mmiri mmiri, uwe aka, na ụdọ ụlọ ọrụ mmepụta ihe.

      • Adhesives maka akpụkpọ ụkwụ na ihe owuwu.

      • Jaketị eriri na mkpuchi elu ụlọ.

    3. Rba Nitrile Hydrogenated (HNBR)

    • Njirimara:

      • Enwetara nguzogide okpomọkụ (ruo +150 Celsius) ma e jiri ya tụnyere NBR.

      • Iguzogide mmanu mmanu, mmiri mmiri hydraulic, na amines.

      • Ike ike dị elu na ike ọgwụgwụ.

      • Obere permeability na gas.

    • Uru:

      • Na-ejigide elasticity n'okpuru mkpughe ogologo oge na kemịkalụ siri ike.

      • Ogologo ndụ dị ogologo karịa NBR n'ọnọdụ dị oke egwu.

    • Ngwa:

      • Ngwá ọrụ na-egwupụta mmanụ na gas (packers, seals).

      • Akara oge ụgbọ ala, ihe ntụtụ mmanụ ọkụ, na akara turbocharger.

      • Ụlọ ọrụ hydraulic cylinders.

    4. rọba silicone (VMQ)

    • Njirimara:

      • Okpomọkụ dị obosara (-60°C ruo +200°C).

      • Ọkpụkpụ dị elu (ruo 1000% elongation).

      • Ezigbo mkpuchi eletrik na nkwụsi ike thermal.

      • Biocompatible na inert.

    • Uru:

      • Na-ejigide mgbanwe na gburugburu cryogenic na oke okpomọkụ.

      • Na-eguzogide UV, ozone, na ihu igwe.

    • Ngwa:

      • Ngwa ahụike (catheters, implants).

      • Ngwa eletrọnịkị (insulators, igodo).

      • gaskets okpomọkụ dị elu maka oven na injin.

    5. Fluorosilicon roba (FVMQ)

    • Njirimara:

      • Na-agwakọta mgbochi kemịkalụ FKM na mgbanwe VMQ.

      • Okpomọkụ dị nso: -50°C ruo +230°C.

      • Na-eguzogide mmanụ ọkụ, lubricants, na mmiri mmiri hydraulic.

      • Ntọala mkpakọ dị ala na nkwụsi ike dị mma.

    • Uru:

      • Na-eme ma na oke okpomọkụ na obere okpomọkụ.

      • Na-eguzogide ọzịza na mmanụ ụgbọ elu.

    • Ngwa:

      • Ihe mejupụtara sistemu mmanụ ụgbọ elu (valvụ, akara).

      • gaskets na njikọ njikọ dị n'oké osimiri submersible.

      • Ihe mmetụta ụgbọ ala na sistemụ njikwa ikuku.

    6. Ethylene Propylene Diene Monomer (EPDM)

    • Njirimara:

      • Ozone pụtara ìhè na nguzogide ihu igwe.

      • Ike dielectric dị elu na nguzogide mmiri.

      • Okpomọkụ dị nso: -50°C ruo +150°C.

      • Obere gas permeability.

    • Uru:

      • Kacha dị ọnụ ahịa maka ngwa n'èzí.

      • Mmanya ịma jijiji na mbelata mkpọtụ.

    • Ngwa:

      • Mkpuchi ihu igwe ụgbọ ala, hoses radiator, na mkpuchi ikuku.

      • Ihe mkpuchi mkpuchi ụlọ na ọdọ mmiri.

      • Igwe mkpuchi ọkụ eletrik na eriri nnyefe ike.


Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Email: 
'); } if ($(obj).parent().next(".errormessage").html() == "") { $(obj).parent().next(".errormessage").html('This field is required').show(); } return false; } else { $(obj).parent().next(".errormessage").html("").hide(); return true; } } } function rEKCDbrgzSiZ_checkFormMail(obj) { if (!rEKCDbrgzSiZ_validateMail($(obj).val())) { if (undefined == $(obj).parent().next(".errormessage").html()) { $(obj).parent().after(' '); } if ($(obj).parent().next(".errormessage").html() == "") { $(obj).parent().next(".errormessage").html('invalid email address').show(); } return false; } else { $(obj).parent().next(".errormessage").html("").hide(); return true; } } function rEKCDbrgzSiZ_validateMail(mail) { var patten = new RegExp(/^([a-zA-Z0-9_\-'])*([\.a-zA-Z0-9_\-'])+@([a-zA-Z0-9_\-'])+((\.[a-zA-Z0-9_\-']+)+)\s*$/); if ($.isEmptyObject(mail) || patten.test(mail)) { return true; } else { return false; } } function subcriptionSubmit(token) { _that = $("." + widget + " #submit"); if ($(_that).hasClass("disableClick")) { return } if (!!token) { if($("."+widget+" #submit").hasClass('FCaptcha')){ var fcToken= token.captchaVerification; $("." + widget + " form").prepend(''); }else { $("." + widget + " form").prepend(''); } } // 互动统计 if (window._ldDataLayer && window._ldDataLayer.push) { var p_sid = $.cookie('p_sid') || 0; var _eventUid = p_sid + widget + new Date().getTime(); window._ldDataLayer.push(["event", "action_formSubmit", "click", "submit", $.trim($("." + widget + " .sitewidget-hd").text()), '', _eventUid]); if ($("." + widget + " form").find('.evuid').length > 0) { $("." + widget + " form").find('.evuid').remove(); } if ($("." + widget + " form").find('._eventReferer').length > 0) { $("." + widget + " form").find('._eventReferer').remove(); } $("." + widget + " form").prepend(''); $("." + widget + " form").prepend(''); } if ($(_that).hasClass("post-loading") || $(_that).hasClass("post-success")) { return false; } var varifyResult = true; $("." + widget + " [required]").each(function () { varifyResult = varifyResult &&rEKCDbrgzSiZ_checkFormEmpty(this); }) $("." + widget + " .mailInput").each(function () { varifyResult = varifyResult &&rEKCDbrgzSiZ_checkFormMail(this); }) if (varifyResult) { $(_that).addClass("disableClick"); $(_that).addClass("post-loading").append(''); var serializeData = $("." + widget + " #mailCollect").serialize(); serializeData = serializeData.replace(/\+/g, " "); serializeData = decodeURIComponent(serializeData); $.ajax({ url: "/phoenix/admin/form", type: "post", data: serializeData, success: function (response, textStatus, jqXHR) { $("." + widget + " #submit").removeClass("post-loading").find(".fa-spinner").remove(); $("." + widget + " #submit").addClass("post-success").append(''); setTimeout(function () { $("." + widget + " #submit").removeClass("post-success").find(".fa-check").remove(); $("." + widget + " .mailInput").val(""); $("." + widget + " .mailInput").blur(); }, 1600); $(_that).removeClass("disableClick") } }); } }