Sesẽ adhesion ami tsitretsitsi hydraulic hose hnbr .
Amadede: Ameyibɔ ƒe
sesẽme: 75-85 shore
Vulcanization ɖoɖo: sulfur ɖoɖo
raw rababa acrylonitrile ƒe agbɔsɔsɔme: 35±3%
lolome: woate ŋu atrɔ asi le eŋu (strip alo keke)
Vulcanization nɔnɔmewo: 170°C*10min secondary vulcanization: 150°C*
4H