resistensia ti kemikal Seal ti resistensia ti lana HNBR .
Kolor:
Nangisit a Kinatangken: 55-65 Shore Ti
sistema ti bulkanisasion: Sistema ti asupre
raw rubber acrylonitrile Linaon: 43±3%
Kadakkel: Mabalin a ma-customize (strip wenno nalawa)
Dagiti kondision ti bulkanisasion: 170°C*10min Sekondario a bulkanisasion: 150°C*4H (2mm Standard a pagsubok a pedaso)
MOQ: 50KGG