Processability ɲuman abrasion resistance triangulaire cɛsirilan HNBR .
Kulɛri: Numukɛ
ka gɛlɛn: 55-65 kɔgɔjida la
vulkanization system: sulfure système
acrylonitrile raw lastikuw hakɛ: 35±3%
A bonya: a bɛ se ka kɛ ka kɛɲɛ ni a yɛrɛ sago ye (a ka bon walima a ka bon)
Vulkanization conditions: 170°C*10min secondaire vulcanization: 150°C*4H (2mm standard test piece)
Moq: 50kg