Sɛnea ɛte ne ne tebea: fitaa (a ɛda adi anaasɛ ɛyɛ nea ɛyɛ mmerɛw) Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 3.9%
Ethylene a ɛwɔ mu: 68.5%
Ngo a wɔde yɛ adwuma: 20%
Mooney Viscosity: ML(1+4)125°C 41
Size: 25kg/block
moq: 25kg
Packed: Boxed
Sɛnea ɛte ne tebea: granules fitaa (transparent anaa translucent)
Monomer a ɛto so abiɛsa no su ne nea ɛwom: ENB,4%
Ethylene dodow: 68.5%
Menni viscosity: ML(1+4)125°C 45
Ne kɛse ne ne nkyerɛkyerɛmu: 25kg/bag
Dodow a ɛba fam koraa a wɔkra: 25kg
Packing: Boxed
Sɛnea ɛte ne ne tebea: fitaa (a ɛda adi anaasɛ ɛyɛ hann) Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 4%
ethylene a ɛwɔ mu: 68.5%
Mooney Viscosity: ML (1+4) 125°C 70
Size: 25kg/bag
MOQ: 25kg
Packing: Boxed: Boxed
Sɛnea ɛte ne ne tebea: fitaa (a ɛda adi anaasɛ ɛyɛ hann) granular
monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 4%
ethylene a ɛwɔ mu: 68.5%
Mooney viscosity: ML (1+4) 125°C 70
Size: 25kg/bag
moq: 25kg
Packing: Boxed: Boxed: Boxed
Sɛnea ɛte ne ne tebea: fitaa (a ɛda adi anaasɛ ɛyɛ hann) Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 7.7%
Ethylene a ɛwɔ mu: 52.5%
Mooney Viscosity: ML(1+4)125°C 65
Size: 25kg/bag
moq: 25kg
Packing: Boxing: Boxing
Sɛnea ɛte ne ne tebea: fitaa (a ɛda adi anaasɛ ɛyɛ hann) Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 7%
ethylene mu nsɛm: 52%
Mooney Viscosity: ML (1+4) 100°C 45
Size: 25kg/bag
moq: 25kg
Packing: Boxed