A cogoya ni a cogoya: finman (a jɛlen don walima a bɛ yeelen bɔ) bloki
Monomɛri suguya sabanan ni a kɔnɔfɛnw: ENB, 4%
Etilɛni hakɛ: 68,5%
Mooney sɔgɔsɔgɔninjɛ: ML (1+4) 125°C 70
Bonya: 25kg/bɔrɔ
MOQ: 25kg
Pake: kɛsu kɔnɔ
A cogoya ni a cogoya: fin (transparent walima translucent) granular
Monomɛri suguya sabanan ni a kɔnɔfɛnw: ENB, 4%
Ethylene hakɛ: 68,5%
Mooney viscosity: ML (1+4) 125°C 70
Bonya: 25kg/bag
MOQ: 25kg
Packing: boxed
A cogoya ni a cogoya: finman (a jɛlen don walima a bɛ yeelen bɔ) bloki
Monomɛri suguya sabanan ni a kɔnɔfɛnw: ENB, 7%
Ethylene hakɛ: 52%
Mooney viscosity: ML (1+4) 100°C 45
Bonya: 25kg/bag
MOQ: 25kg
Packing: boxed