Inkinga yokungcoliswa kwesikhunta yinto evamile embonini yokucubungula irabha. Ungqimba lwamadiphozi luyakha ezindongeni zesikhunta ngesikhathi senqubo ye-vulcanization futhi kancane kancane lunqwabelana phakathi nomjikelezo wokukhiqiza olandelayo. Izincwadi zangaphambilini zixoxile ngethonya lezici ezihlukahlukene ezibangela ukukhunta kwesikhunta. Manje sekutholakele ukuthi kuma-vulcanizate ahlukahlukene (kanye ne-zinc oxide) equkethwe kumakhompiyutha enjoloba e-polymeric, i-zinc sulfide iwumkhiqizo wokusabela ocasula kakhulu wenqubo ye-vulcanization ebangela ukungcoliswa. Asikho i-ejenti yokukhishwa ehlala unomphela noma imbondela engunaphakade (yensimbi) engagwema lokhu kubekwa. Isiphetho siwukuthi ukungcola ekuqaleni kubangelwa i-zinc sulfide (ama-inorganic deposits) enamathela esikhunjeni futhi yakhe ungqimba lwediphozithi olumpunga. Njengomsebenzi wokushisa, izingxenye eziphansi zesisindo samangqamuzana engxube zinamathela kuma-microcrystals e-zinc sulfide futhi zibangele isigaba sesibili sokubeka (i-organic deposition). Imikhiqizo ye-oxidation yakhiwa phakathi nesikhathi esithile futhi ibangele ukubekwa kwekhabhoni.
Ngokuqonda izimbangela zokungcoliswa kwesikhunta kanye nezinqubo ezitholakala ekwakhekeni kwe-zinc sulfide microcrystals endaweni yensimbi yesikhunta, kungenzeka ukukhiqiza indlela esebenzayo ekucubunguleni kwamanje ukuze kuncishiswe ukwakheka kwe-zinc sulfide futhi ngaleyo ndlela kuvimbele ukungcoliswa kwesikhunta. Ngokutadisha izimbangela zokungcola, kungenzeka ukunciphisa lesi simo. Kunezixazululo ezimbili ezingenzeka zokuvimbela noma ukunciphisa ukwakheka kokungcola : shintsha ukwakheka kwengxube noma uthuthukise ubuso bokufa. Ukushintsha ukwakheka kwengxube ukuze kuncishiswe ukungcola ngenxa ye-zinc oxide noma inhlanganisela ye-sulfide kumele kuncishiswe noma kuqedwe. Amadiphozithi amaningi ahlotshaniswa namazinga aphezulu e-vulcanization kanye ne-zinc oxide, evame ukusetshenziswa emikhiqizweni yenjoloba yamasondo. Amathayi yiwona omkhulu wemikhiqizo yenjoloba yomhlaba wonke ngevolumu (kufika ku-75%). Ngakho-ke, ucwaningo oluningi lwenziwa ngezingxube ze-NR/BR compounds nezinhlanganisela ze-SBR ezivame ukusetshenziswa ekukhiqizeni amathayi. Umthelela we-zinc vulcanization, ukuhlolwa kwe-vulcanization yesikhashana esifushane, kanye nomthelela wokubunjwa okuhlanganisiwe kwahlolwa ngokwemibandela yokunciphisa isikali sesikhunta ngokushintsha ukwakheka kwengxube.