Ponahalo: phofo e mosehla e bobebe
Znic oxide Content:min 50%
Active Znic oxide Content:min.93%
Sebaka se khethehileng sa sebaka: 25m2 / g
density: 3.4g/cm3
Ponahalo: phofo e mosehla e bobebe
Znic oxide Content:min 54%
Active Znic oxide Content:min.93%
Sebaka se khethehileng sa holim'a metsi: 20-30m2 / g
density: 3.6g / cm3