Cold Resistance Rapid Vulcanization Suauu-tumu Ethylene Propylene Rubber-EPDM

Faʻaaliga ma tulaga: Beige poʻo samasama lanu samasama poloka
lona tolu monomer ituaiga ma anotusi: ENB, 8.5%
Ethylene anotusi: 52.5%
Mooney viscosity: ML (1 + 4) 125 ° C 68
Suauʻu mea: 20%
Tele: 25kg / poloka
MOQ: 25kg
afifi: pusa
  • TER 8148

Avanoa:
Tele:

' Fa'asa'o Ma'alili ma Vave Vulcanization Ethylene Propylene Rubber-EPR TER 8148: O le Fofo Sili mo Talosaga Eseese'

Keywords:
1. Tete'e malulu
2. Fa'asao vave
3. Fa'atumu suau'u
4. Siosiomaga
5. Anti-vibration
6. Insulation leo
7.
fa'amalieina lelei.
Fa'amaumau tau fa'amautu 8. Sone
Folasaga

:
Fa'ailoaina o le Ethylene Propylene Rubber-EPR TER 8148, o se mea fou e tu'ufa'atasia ai le malulu, fa'asao vave, fa'atumuina o mea totino, fa'afeiloa'iga o le si'osi'omaga, fa'ama'i-vibration, fa'amama leo, tau maualalo, mautu lelei, fa'aoso fa'amau, ma fa'asagaga o le osone. O lenei pa'u pa'u felagolagoma'i ua mamanuina e fa'amalieina mana'oga mana'omia o alamanuia eseese, ofoina atu fa'atinoga fa'apitoa ma fa'amaoni.

Tete'e malulu:
EPR TER 8148 fa'aalia le mata'ina o le tete'e malulu, fa'amautinoaina lona fa'atinoina lelei e o'o lava i tulaga ogaoga o le vevela. O lona gafatia e tausia ana mea faʻaletino ma faʻainisinia i le maualalo o le vevela e lelei ai mo faʻaoga i totonu o siosiomaga faigata lea e sili ona taua le tumau ma le fetuutuunai.

Vave Vulcanization:
Fa'atasi ai ma ona uiga fa'apitoa fa'asao fa'asao, EPR TER 8148 fa'ataga mo faiga fa'anatinati vave ma lelei. O lona tu'ufa'atasiga tulaga ese o vaila'au e mafai ai ona vave feso'ota'i, fa'aitiitia le taimi fa'amalolo e aunoa ma le fa'afefeteina o mea lelei. O lenei vaega e sili ona aoga mo alamanuia o loʻo i ai faʻatonuga faʻatulagaina o gaosiga ma maualuga manaʻoga.

Su'u-Faatumu:
EPR TER 8148 o se pa'u fa'atumu-tumu suau'u, e maua ai le malosi fa'afefete ma fa'amavaega. O lona malosi fa'anatura e mitiia ma fa'ate'a ese le te'i ma le malosi o le vibration e fa'amalieina mo talosaga e mana'omia ai le fa'aitiitia o le pisa ma fa'aleleia atili le fa'amafanafanaga, e pei o totonu o ta'avale, masini fa'apipi'i, ma le fa'amama leo.

Fa'alesiosiomaga:
Fuafuaina ma le gafataulimaina i le mafaufau, EPR TER 8148 ua fa'atulagaina e fa'aoga ai mea e fa'alelei i le si'osi'omaga ma fa'agaioiga gaosiga. O lona fa'aitiitia o tulagavae kaponi ma le la'ititi o le a'afiaga o le si'osi'omaga ua avea ai ma filifiliga aulelei mo kamupani o lo'o naunau i le fa'afoeina o puna'oa fa'atatau ma fa'aitiitia o latou tulagavae fa'alenatura.

Anti-Vibration and Sound Insulation:
EPR TER 8148 e ofoina atu le maualuga o le anti-vibration ma le leo fa'amalu, fa'amama lelei le fa'afefeteina mai fafo ma fa'aitiitia le pisa. O lona malosi fa'asusu e maua ai se si'osi'omaga e sili atu le filemu ma sili atu le fa'alelei o galuega po'o le nofo ai, ma fa'amalieina mo masini ma'ale'ale ma avanoa e mana'omia ai le pulea o le pisa.

Tau maualalo:
E ui lava i lona tulaga faʻapitoa ma foliga faʻapitoa, EPR TER 8148 o loʻo ofoina atu i se tau tauva. O lona natura taugofie e mafai ai ona maua e le tele o alamanuia, e mafai ai ona latou manuia mai ona tulaga lelei e aunoa ma le gau o le faletupe.

Lelei Faʻamautu Faʻamau ma Faʻamau Seti Resistance:
EPR TER 8148 faʻaalia lelei tulaga mautu, tausia lona foliga ma fua i lalo o le eseese o le vevela ma mamafa. O lona teteʻe atu i seti faʻapipiʻi e faʻamautinoa ai le umi o le faʻatinoga ma faʻamaufaʻailoga faʻatuatuaina talosaga, faʻamaonia mo vaega taua i fale taʻavale, fale gaosi oloa, ma fale faufale.

Tete'e o le Osone:
Fa'amaualuga le malosi o le tete'e o le osone, EPR TER 8148 e tetee atu i a'afiaga leaga o le fa'aalia o le osone e aunoa ma le fa'aleagaina. O lona gafatia e tetee atu i le faʻaleagaina o le oxidative e faʻamautinoa ai le faʻatuatuaina o le faʻatinoga i siosiomaga i fafo ma fesoasoani i le faʻalauteleina o le ola o oloa.

Fa'ai'uga:
O le Ethylene Propylene Rubber-EPR TER 8148 o lo'o tu i fafo o se mea fa'apitoa ma fa'atuatuaina e tu'ufa'atasia ai le malulu, fa'asao vave, fa'atumu o le suau'u, fa'afeiloa'iga o le si'osi'omaga, anti-vibration, insulation leo, tau maualalo, mautu tulaga lelei, fa'apipi'i seti tete'e, ma ozone tetee. Pe o oe i totonu o fale gaosi oloa, su'e vaifofo tu'ufua vibration, pe mana'omia mea mo tulaga vevela vevela, EPR TER 8148 e tu'uina atu le fa'atinoga ma le taua. Talia le aoga o lenei pa'u fou fou ma iloa le eseesega e mafai ona faia i au galuega faatino.

Muamua: 
Sosoo ai: 

SO'OGA VAIVAI

OA TATOU Oloa

FA'AALIGA FESOASOANI

Faʻaopoopo: Nu.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telefoni / WhatsApp / Skype: +86 15221953351
Puletaofia     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Faiga Fa'alilolilo | Lagolago e Leadong.