ENB Ntoya MWD TPO Ethylene Propylene Rubber-EPDM
Kugaragara no kumiterere: cyera (kibonerana cyangwa gisobanutse) kibuza
Ubwoko bwa gatatu bwa monomer n'ibirimo: ENB, 1.0%
Ibirimo Ethylene: 66%
Ubukonje bwa Mooney: ML (1 + 4) 125 ° C 46
Ingano: 25kg / guhagarika
MOQ: 25kg
Gupakira: agasanduku