Ọdịdị na ọnọdụ: ọcha (transperent ma ọ bụ translucent) blocky
Ụdị monomer nke atọ na ọdịnaya: ENB, 4.5%
Ethylene ọdịnaya: 69%
Mooney viscosity: ML (1 + 4) 125 ° C 63
Size: 25kg / igbochi
MOQ: 25kg
Mbukota: boxed
Ọdịdị na ọnọdụ: ọcha (transperent ma ọ bụ translucent) blocky
Ụdị monomer nke atọ na ọdịnaya: ENB, 6.5%
Ethylene ọdịnaya: 68%
Mooney viscosity: ML (1 + 4) 125 ° C 135
Size: 25kg / igbochi
MOQ: 25kg
Mbukota: boxed
Ọdịdị na ọnọdụ: ọcha (transparent ma ọ bụ translucent) blocky
Ụdị monomer nke atọ na ọdịnaya: ENB, 4.1%
Ethylene ọdịnaya: 53%
Mooney viscosity: ML (1 + 4) 125 ° C 30
Size: 25kg / igbochi
MOQ: 25kg
Mbukota: boxed
Ọdịdị na ọnọdụ: ọcha (transperent ma ọ bụ translucent) blocky
Ụdị monomer nke atọ na ọdịnaya: ENB, 1.0%
Ethylene ọdịnaya: 66%
Mooney viscosity: ML (1 + 4) 125 ° C 46
Size: 25kg / igbochi
MOQ: 25kg
Mbukota: boxed