Mooney Viscosity Amavuta yuzuye Hose Ethylene Propylene Rubber-EPR
Kugaragara no kumiterere: byera (bisobanutse cyangwa bisobanutse) byahagaritswe
Ubwoko bwa gatatu bwa monomer n'ibirimo: ENB, 5.7%
Ibirimo Ethylene: 70%
Ibirimo amavuta: 50%
Ubukonje bwa Mooney: ML (1 + 4) 125 ° C 53
Ingano: 25kg / guhagarika
MOQ: 25kg
Gupakira: agasanduku