A cogoya ni a cogoya: finman (a jɛlen don walima a bɛ yeelen bɔ) bloki
Monomɛri suguya sabanan ni a kɔnɔfɛnw: ENB, 9%
Ethylene hakɛ: 60%
Mooney viscosity: ML(1+4)125°C 92
Bonya: 25kg/block
MOQ: 25kg
Packing: boxed
A cogoya ni a cogoya: fin (transparent walima translucent) blocky
Monomɛri suguya sabanan ni a kɔnɔfɛnw: ENB, 8,5%
Ethylene hakɛ: 60%
Mooney viscosity: ML (1+4) 125°C 84 ML(1+4)150°C 81
Bonya: 25kg/block
MOQ: 25kg
Packing: boxed