Fanovàna plastika mahery vaika Ethylene Propylene Rubber-EPR
Karazana: Fingotra ethylene propylène binary
Ny endriny sy ny toe-javatra: fotsy (mangarahara na mangarahara) mipetaka
Ethylene votoaty: 52%
Propylene votoaty: 48%
Mooney viscosity: ML (1+4) 100°C 80
Habe: 25kg/kitapo
MOQ: 25kg