Giga Agbara Ṣiṣu Iyipada Ethylene Propylene Rubber-EPR
Iru: Alakomeji ethylene propylene roba Irisi
ati ipo: funfun (sihin tabi translucent) blocky
Ethylene akoonu: 52%
Propylene akoonu: 48%
Mooney viscosity: ML (1 + 4) 100 ° C 80
Iwọn: 25kg / apo
MOQ: 25kg
Iṣakojọpọ: apoti