A lan dan leh a dinhmun: Beige emaw pale yellow blocky
Third monomer chi leh a awm zat: ENB, 4.5%
Ethylene awm zat: 59.5%
Mooney viscosity: ML(1+4)125°C 47
Oil awm zat:10%
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: Beige emaw pale yellow blocky
Third monomer chi leh a awm zat: ENB, 4.5%
Ethylene awm zat: 55.5%
Mooney viscosity: ML(1+4)125°C 55
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: Beige emaw pale yellow blocky
Third monomer chi leh a awm zat: ENB, 7%
Ethylene awm zat: 53%
Mooney viscosity: ML(1+4)125°C 65
Oil awm zat: 18%
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: Beige emaw pale yellow blocky
Third monomer chi leh a awm zat: ENB, 8.5%
Ethylene awm zat: 52.5%
Mooney viscosity: ML(1+4)125°C 68
Oil awm zat:20%
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: Beige emaw pale yellow blocky
Third monomer chi leh a awm zat: ENB, 7.4%
Ethylene awm zat: 60.6%
Mooney viscosity: ML(1+4)125°C 33
Oil awm zat: 30%
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: Beige emaw pale yellow blocky
third monomer chi leh a thupui: ENB, 4.5%
Ethylene awm zat: 55.5%
Mooney Viscosity: ML(1+4)125°C 76
Size: 25kg/block
MOQ: 25KG
Packing: Boxed