Ku languteka na xiyimo: Beige kumbe pale yellow blocky
Muxaka wa vunharhu wa monomer na nhlayo: ENB, 3.4%
Ethylene: 64.6%
Mooney viscosity: ML(1+4)125°C 32
Nhlayo ya oyili: 100%
Vukulu: 25kg/block
MOQ: 25kg
Ku paka: boxed
Ku languteka na xiyimo: Beige kumbe pale yellow blocky
third monomer muxaka na nhundzu: ENB, 8.5%
ethylene content: 52.5%
Mooney viscosity: ML(1+4)125°C 68
mafurha ya le ndzeni: 20%
Vukulu: 25kg/block
MOQ: 25kg
Packing:
Ku languteka na xiyimo: Beige kumbe muhlovo wo tshwuka wo tshwuka wa blocky
muxaka wa monomer wa vunharhu na nhundzu: ENB, 4.5%
Nhlayo ya le henhla: 55.5%
Mooney Viscosity: ML(1+4)125°C 55
Vukulu:
25kg/block MOQ
Ethylene
Ku languteka na xiyimo: Beige kumbe pale yellow blocky
Muxaka wa vunharhu wa monomer na nhlayo: ENB, 4.7%
Ethylene: 68.3%
Mooney viscosity: ML(1+4)125°C 28
Nhlayo ya oyili: 43%
Vukulu: 25kg/block
MOQ: 25kg
Ku paka: boxed