Minimum ENB Narrow MWD TPO Ethylene Propylene Flexilis-EPDM
Aspectus et conditio: album (perlucidum vel translucidum) obstupefactum
tertium genus monomerorum et contentum: ENB, 1.0%
Ethylene content: 66%
viscositas Mooney: ML (1+4) 125°C 46
Magnitudo: 25kg/obstructionum
MOQ: 25kg
sarcina: cohibenti