Tare da shekaru na gwaninta a cikin samarwa
Ethylene Propylene Diene Rubber ,
Herchy na iya samar da nau'i mai yawa na
Ethylene Propylene Diene Rubber .
Ethylene Propylene Diene Rubber zai iya saduwa da aikace-aikacen da yawa, idan kuna buƙatar, don Allah sami sabis na kan layi akan lokaci game da
Ethylene Propylene Diene Rubber . Baya ga jerin samfuran da ke ƙasa, Hakanan zaka iya keɓance na musamman
Ethylene Propylene Diene Rubber bisa ga takamaiman bukatunku.
Bayyanawa da yanayin: fari (m ko mai bayyanawa) toshe
Nau'in monomer na uku da abun ciki: ENB, 5.0%
abun ciki na Ethylene: 64%
abun ciki na mai: 75%
dankon Mooney: ML (1 + 4) 125 ° C 55
Girman: 25kg / toshe
MOQ: 25kg
Packing: 25kg Packing
Bayyanawa da yanayin: fari (m ko mai bayyanawa) toshe
Nau'in monomer na uku da abun ciki: ENB, 1.0%
Ethylene abun ciki: 66%
Mooney danko: ML (1 + 4) 125 ° C 46
Girman: 25kg / toshe
MOQ: 25kg
Packing: akwati
Bayyanawa da yanayin: fari (mai bayyana ko m) toshe
Nau'in monomer na uku da abun ciki: ENB, 4.1%
Ethylene abun ciki: 53%
Mooney danko: ML (1 + 4) 125 ° C 30
Girman: 25kg / toshe
MOQ: 25kg
Packing: akwati