Mooney ka bon fanga ka bon granulated Ethylene Propylene Rubber-EPR

A cogoya ni a cogoya: fin (transparent walima translucent) granular
Monomɛri sabanan suguya ni a kɔnɔfɛnw: ENB, 4%
Ethylene hakɛ: 68,5%
Mooney viscosity: ML (1+4) 125°C 70
Bonya: 25kg/bag
MOQ: 25kg
Packing: boxed
  • J-3080P ye

Disponibilité:
Hakɛ:
High Mooney High Strength Granulated Ethylene Propylene Rubber-EPR Raw Rubber

Daminɛ:
An ka High Mooney High Strength Granulated Ethylene Propylene Rubber-EPR Raw Rubber ye fɛn ye min bɛ se ka kɛ fɛn caman ye, min dilannen don baara suguya caman kama. Ni a ka Mooney sɔgɔli ka bon, a fanga danfaralen, ani a cogo granulaire, a bɛ nafa caman di baarakɛcogo ɲuman ni fɛn caman kɛcogo la.

I. Baarakɛcogo ɲuman sabatili :
An ka EPR lastikuw sɛnɛcogo granulaire bɛ nɔgɔya ni baarakɛcogo ɲumanba di baarakɛcogo la. Ni i y’a suma ni laadala sɛbɛnfura walima bloki cogoyaw ye, granules bɛ kɛ sababu ye ka sumani, minɛni ani jateminɛ nɔgɔya, o la, a dilanni taabolo bɛ nɔgɔya. Granules bonya ni u cogoya kelen bɛ a to fɛnw tilatilali bɛ kɛ cogo kelen na ani ka tiɲɛni dɔgɔya.

II. Fɛnɲɛnamafagalanw jɛnsɛnni ka ɲɛ :
An ka EPR lastikuw sɛnɛcogo granulaire bɛ jɛnsɛnni ɲɛnabɔli nɔgɔya fɛnɲɛnamafagalanw kɔnɔ. Ni fɛnɲɛnɛmaw hakɛ ka dɔgɔn, o bɛ kɛ sababu ye ka fɛn in tila-tila ka ɲɛ, o bɛ na ni a ɲagaminen ye cogo kelen na ani ka fɛn laban kɛcogo ɲɛ. O bɛ dɔ fara baarakɛcogo labanw baarakɛcogo bɛɛ kan ani u ka ɲumanya kan.

III. Teliya la, a wulicogo ni a ɲagamini :
An ka EPR lastikuw sɛnɛcogo granulaire bɛ wulicogo ɲuman jira, o b’a to a bɛ se ka wuli kosɛbɛ ani ka ɲagami ɲɔgɔn na. Granules bɛ wuli joona ani cogo kelen na ni u kɛra funteni na, o bɛ kɛ sababu ye ka u ɲagami ka ɲɛ ni faralifɛn wɛrɛw ye ani fɛnɲɛnamafagalanw ye. O se min bɛ kɛ ka wuli teliya la, o bɛ baara kɛ waati bɛɛ ɲɛ ani ka fɛnɲɛnamafagalanw dilancogo kelenw sabati.

IV. A bɛ se ka kɛ fɛn caman ye ani a bɛ se ka ladamu:
An ka EPR lastikuw ka granular nature bɛ fɛn caman kɛ ani ka ladamu fɛn dilanni taabolo suguya caman na. A bɛ se ka don nɔgɔya la pikiri dilanni, bɔli, walima kalolabɔ baara la, o bɛ kɛ sababu ye ka fɛn caman kɛ. Granules bɛ sira di ka fɛnw hakɛ kɔlɔsi tigitigi ani ka a to baarakɛcogo bɛ kɛ cogo kelen na sɛnɛ kɛcogo wɛrɛw la.

Kuncɛli :
An ka High Mooney High Strength Granulated Ethylene Propylene Rubber-EPR Raw Rubber bɛ granular cogo di min bɛ nafa caman di baarakɛcogo ɲuman ni baarakɛcogo caman na. Granules bɛ se ka kɛ sababu ye ka u minɛ ka ɲɛ, ka u jɛnsɛn ka ɲɛ, ani ka wuli joona ani ka u ɲagami. O bɛ dɔ fara baarakɛcogo labanw ka baarakɛcogo ɲuman kan, u ka ɲumanya, ani u ka baarakɛcogo bɛɛ lajɛlen na. A ka baarakɛcogo caman n’a bɛ se ka ladamu, an ka EPR lastikuw sɔgɔlenw bɛ baara sɔrɔ izini suguya caman na, o b’a to a ye sugandili ɲuman ye dilanbagaw bolo minnu bɛ baarakɛcogo ɲuman ɲini ani fɛn laban minnu bɛ se ka da u kan.
Tɛmɛnen: 
Nata: 

LINKS TELIKANW

AN KA FƐƐRƐW

KUNNAFONIW MINNU BƐ SƆRƆ

A farala: No.33, Lane 159, Taiye sira kan, Fengxian mara la, Shanghai
Telefɔni / WhatsApp / Skype: +86 15221953351
Hakilila-jɔ-sɛbɛn     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap (yɔrɔ karti). |   Kunnafoni dogolenw ka sariya | Dɛmɛn By Leadong ye.