Sɛnea ɛte ne ne tebea: Beige anaa Pale Yellow Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 4.5%
Ethylene a ɛwɔ mu: 63.5%
Mooney Viscosity: ML(1+4)125°C 57
Ngo a ɛwɔ mu: 67%
kɛse: 25kg/block
MOQ: 25kg
Packing: Boxed
Sɛnea ɛte ne ne tebea: Beige anaa Pale Yellow Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 4.4%
Ethylene Nsɛm: 68.6%
Mooney Viscosity: ML(1+4)125°C 77
Size: 25kg/block
MOQ: 25kg
Packing: Boxed
Sɛnea ɛte ne ne tebea: Beige anaa Pale Yellow Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 8.9%
Ethylene Nsɛm: 60.1%
Mooney Viscosity: ML(1+4)100°C 64
Size: 25kg/block
MOQ: 25kg
Packing: Boxed
Sɛnea ɛte ne ne tebea: Beige anaa Pale Yellow Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 5.5%
Ethylene a ɛwɔ mu: 66.5%
Mooney Viscosity: ML(1+4)125°C 43
Ngo a ɛwɔ mu: 67%
kɛse: 25kg/block
MOQ: 25kg
Packing: Boxed
Sɛnea ɛte ne ne tebea: Beige anaa Pale Yellow Blocky
Monomer a ɛto so abiɛsa no su ne emu nsɛm: ENB, 4.4%
Ethylene Nsɛm a ɛwom: 68.6%
Mooney Viscosity: ML(1+4)125°C 60
Size: 25kg/block
MOQ: 25kg
Packing: Boxed