Wowɔ ha: Fie » Ano aduru . » Ano aduru . » Sɛnea wobɛma rɔba ahoɔden a ɛyɛ den no atu mpɔn wɔ ɔhyew a ɛkɔ soro mu

Sɛnea wobɛma rɔba ahoɔden a ɛyɛ den no atu mpɔn wɔ ɔhyew a ɛkɔ soro mu .

Ɛwom sɛ ade a wɔde nkata so no betumi adi nea ɔde di dwuma no ahwehwɛde ahorow a ɛfa ahoɔden a ɛtwetwe ade ho wɔ dan mu hyew mu no ho dwuma de, nanso nea ɔde di dwuma no bebisa ahoɔden a ɛtwetwe no wɔ ɔhyew a ɛkorɔn bi mu bere a ɔresusuw sɛnea ade no yɛ adwuma wɔ ɔhyew a ɛkɔ soro mu, a ɛnyɛ bere nyinaa na ebetumi ayɛ yiye no. Ɛyɛ den sɛ wobedi adetɔfo ahwehwɛde yi ho dwuma.

1. Silicone rɔba .

Wɔ ɔhyew a ɛkɔ soro yiye mu no, silicone rɔba ma ɔhyew a ɛkɔ soro tensile ahoɔden sen organic elastomers afoforo nyinaa.

2. SBR .

NR ne SBR a wɔde frafra mu wɔ 50:50 ratio (mass ratio) mu no ma SBR nnuru a ɛyɛ hyew a ɛkɔ soro no yɛ adwuma yiye.

3. EPDM .

Ziegler-Natta Catalytic mfiridwuma no ma ethylene no yɛ hyew kɛse wɔ ɔhyew a ɛkɔ soro wɔ EPDM mu, na ɛma ɔhyew a ɛkɔ soro a ɛma ɛyɛ den. Sɛ wogyina sɛnea ethylene no yɛ nhyehyɛe wɔ nhyehyɛe pa mu so a, crystallisation bi fa crystalline nhyehyɛe nsakrae ahorow pii mu wɔ ɔhyew a ɛboro 75°C so.

4. Neoprene CR .

Wɔ CR-gyina adhesives ho no, wɔde W-type neoprene di dwuma, a wɔde silica a wɔatɔ no kɛse ne polyethylene glycol (PEG) dodow a ɛwɔ afã 2 ka ho ma ɛma ade a wɔde kyekyere no nya ahoɔden a ɛkɔ soro wɔ ɔhyew a ɛkɔ soro mu.

5. Silica .

Wɔ tebea horow bi mu no, afã horow 10-20 a silica a ɛtɔ gu so no dodow nam so betumi ama ɔhyew a ɛkɔ soro no ayɛ den ne sɛnea ɛte wɔ adhesive no ho.

Links a ɛyɛ ntɛm .

Yɛn nneɛma .

Nsɛm a wɔde di nkitaho .

Fa ka ho: No.33, Lane 159, Taiye kwan so, Fengxian Mantam, Shanghai .
Tel / WhatsApp / Skype: +8615221953351 .
Nsɛm a ɛfa ho     2023 Shanghai Herchy Rubber Co., Ltd. SiteMap . |   Nsɛm a Wɔde Sie Ho Nsɛm | Mmoa a wɔde ma denam . Leang ..