Ponagalo le mmušo: di-granule tše tšhweu (tše di bonagalago goba tše di bonagalago gabotse)
Mohuta le diteng tša monomer ya boraro: ENB,4%
Diteng tša Ethylene: 68.5%
Viscosity ya Menni: ML(1+4)125°C 45
Bogolo le ga tlhaloso: 25kg/mokotla
Palo ya otara ya fasefase: 25kg
Packing: Boxed