Hitsura at Kondisyon: Puti (Transparent o Translucent) Granular
Third Monomer Type at Nilalaman: ENB, 4%
Ethylene Nilalaman: 68.5%
Mooney Viscosity: ML (1+4) 125 ° C 70
Sukat: 25kg/Bag
MOQ: 25kg
Packing: Boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 4.6%
Ethylene Nilalaman: 57.2%
na singil ng langis: 20%
Mooney Viscosity: ML (1+4) 125 ° C 60
Sukat: 25kg/Bag
MOQ: 25kg
Packing: Boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 7%
Ethylene Nilalaman: 52%
Mooney Viscosity: ML (1+4) 100 ° C 45
Sukat: 25kg/Bag
MOQ: 25kg
Packing: Boxed