Te ahua me te ahua: Beige or kowhai kowhai paraka
Tuatoru momo monomer me te ihirangi: ENB, 5%
Ethylene content: 70%
Mooney viscosity: ML(1+4)100°C 30
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: Beige or kowhai kowhai paraka
Tuatoru momo monomer me te ihirangi: ENB, 4.7%
Ethylene content: 68.3%
Mooney viscosity: ML(1+4)125°C 28
Te hinu hinu: 43%
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: Beige or kowhai kowhai paraka
Tuatoru momo monomer me te ihirangi: ENB, 4.4%
Ethylene ihirangi: 68.6%
Mooney viscosity: ML(1+4)125°C 60
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: Beige or kowhai kowhai paraka
Tuatoru momo monomer me te ihirangi: ENB, 5.5%
Ethylene content: 66.5%
Mooney viscosity: ML(1+4)125°C 43
Te hinu hinu: 67%
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: Beige or kowhai kowhai paraka
Tuatoru momo monomer me te ihirangi: ENB, 8%
Ethylene content: 60%
Mooney viscosity: ML(1+4)125°C 43
Te hinu hinu: 100%
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka