Te ahua me te ahua: Beige or kowhai kowhai paraka
Tuatoru momo monomer me te ihirangi: ENB, 4.5%
Ethylene content: 59.5%
Mooney viscosity: ML(1+4)125°C 47
Te hinu hinu: 10%
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: Beige or kowhai kowhai paraka
Tuatoru momo monomer me te ihirangi: ENB, 7%
Ethylene content: 53%
Mooney viscosity: ML(1+4)125°C 65
Te hinu hinu: 18%
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: Beige or kowhai kowhai paraka
Tuatoru momo monomer me te ihirangi: ENB, 8.5%
Ethylene content: 52.5%
Mooney viscosity: ML(1+4)125°C 68
Te hinu hinu: 20%
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: Beige or kowhai kowhai paraka
Tuatoru momo monomer me te ihirangi: ENB, 5%
Ethylene content: 70%
Mooney viscosity: ML(1+4)100°C 30
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: Beige or kowhai kowhai paraka
Tuatoru momo monomer me te ihirangi: ENB, 4.7%
Ethylene content: 68.3%
Mooney viscosity: ML(1+4)125°C 28
Te hinu hinu: 43%
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka