A ɲɛda ni a cogoya: Beige walima pale jaune blocky
sabanan monomɛri suguya ani a kɔnɔkow: ENB, 3,4%
etilɛni hakɛ: 64,6%
Mooney Viscosité: ml(1+4)125°C 32
Tulu hakɛ: 100%
bonya: 25kg/block
moq: kilo 25
Packing: Boxed
A ɲɛda ni a cogoya: Beige walima pale jaune blocky
sabanan monomɛri suguya ani a kɔnɔkow: ENB, 4,4%
etilɛni hakɛ: 68,6%
Mooney Viscosité: ML(1+4)125°C 77
A bonya: 25kg/block
MOQ: 25kg
Packing: Boxed