Di we aw i tan ɛn di kɔndishɔn: Bij ɔ pale yɔlɔ blɔk
Tɔd monoma tayp ɛn kɔntinyu: ENB, 3.4%
Ɛtilin kɔntinyu: 64.6%
Mooney viskɔsiti: ML(1+4)125°C 32
Ɔyl kɔntinyu: 100%
Sayz: 25kg/blɔk
MOQ: 25kg
Pak: bɔks
Di we aw i tan ɛn di kɔndishɔn: Bij ɔ pale yɔlɔ blɔk
Tɔd monoma tayp ɛn kɔntinyu: ENB, 4.5%
Ɛtilin kɔntinyu: 55.5%
Mooney viskɔsiti: ML(1+4)125°C 55
Sayz: 25kg/blɔk
MOQ: 25kg
Pak: bɔks
Di we aw i tan ɛn di kɔndishɔn: Bij ɔ pale yɔlɔ blɔk
Tɔd monoma tayp ɛn kɔntinyu: ENB, 8.5%
Ɛtilin kɔntinyu: 52.5%
Mooney viskɔsiti: ML(1+4)125°C 68
Ɔyl kɔntinyu:20%
Sayz: 25kg/blɔk
MOQ: 25kg
Pak: bɔks