Herchy hi China lama hmahruaitu a ni .
LEV siamtu, supplier leh exporter Product quality tha famkim zawn zawm a, chutiang chuan kan
LEV chu customer tam takin an satisfy tawh a ni. Extreme design, quality raw materials, high performance leh competitive price te hi customer zawng zawng duh ber a ni a, chu chu kan pe thei bawk che u a ni. Dik tak chuan, a pawimawh bawk chu kan after-sales service ṭha famkim hi a ni. Kan i ngaihven chuan
LEV services tunah hian min rawn zawt thei ang, a hun takah kan chhang ang che!
A lan dan leh a dinhmun: Beige emaw pale yellow blocky
Third monomer chi leh a awm zat: ENB, 4.5%
Ethylene awm zat: 59.5%
Mooney viscosity: ML(1+4)125°C 47
Oil awm zat:10%
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: Beige emaw pale yellow blocky
Third monomer chi leh a awm zat: ENB, 5.5%
Ethylene awm zat: 66.5%
Mooney viscosity: ML(1+4)125°C 43
Oil awm zat: 67%
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: Beige emaw pale yellow blocky
Third monomer chi leh a awm zat: ENB, 4.4%
Ethylene awm zat: 68.6%
Mooney viscosity: ML(1+4)125°C 60
Size: 25kg/block
MOQ: 25kg
Packing: boxed
A lan dan leh a dinhmun: Beige emaw pale yellow blocky
Third monomer chi leh a awm zat: ENB, 8.9%
Ethylene awm zat: 60.1%
Mooney viscosity: ML(1+4)100°C 64
Size: 25kg/block
MOQ: 25kg
Packing: boxed