Views: 0 Omuwandiisi: Site Editor Obudde bw'okufulumya: 2023-08-13 Ensibuko: Ekibanja
Oluvannyuma lw’okuzinga kapiira ka chloroprene ku mizingo, embeera y’ekintu kya kapiira, okufaananako kapiira ak’obutonde, ekyuka n’ebbugumu . Chloroprene rubber phase changes at different temperatures.... By the temperature-induced changes in the rubber between the three states is reversible, mu mbeera ya pulasitiika eya kapiira, singa ebbugumu likendeezebwa, esobola okugifuula okudda mu mbeera ya laasitiki. Nga tukozesa empalirizo y’okusala (shear force) ey’embeera ya laasitiki, ekijjuza kisobola okusaasaanyizibwa obulungi. Ebbugumu ly’okulongoosa kapiira lya chloroprene bwe liba waggulu okusinga 90 °C, ekitundu kya kapiira ka chloroprene kikyusibwa ne kifuuka embeera ya pulasitiika, ekikola okubeera awamu kw’embeera ya laasitiki n’embeera ya pulasitiika, kwe kugamba, embeera ya granular. Nga ebbugumu ly’embeera ya laasitiki eya kapiira ka chloroprene bwe liri wansi okusinga erya kapiira ak’obutonde, bwe kityo ebbugumu lyayo ery’okukola okutabula lirina okuba wansi okusinga erya kapiira ak’obutonde. Mu nkola entuufu ey’ekkolero, ebbugumu ly’okutabula kapiira okutwalira awamu liri waggulu nnyo, kale lirina okuba nga bukyali nga bwe kisoboka okugatta ekijjuza, olwo ekijjuza mu mbeera ya laasitiki okutuuka ku ddaala eritali limu ery’okutabula, okusobola okulongoosa obugumu bw’okutabula kapiira, okwongera ku maanyi g’okusala, bwe kiba mu mbeera y’obuveera ey’okutabula, naye era kisobola okusaasaana obulungi.
( I ) okutabula mu kyuma ekiggule
chloroprene rubber okutabula ebbugumu okusinga natural rubber, kale batch ya chloroprene rubber okutabula okubeera entono katono.
Okutuusa nga kwongerako hard filler, yandibadde cooled roller, okukakasa nti elastic state esobola okugattibwako. Naye magnesium oxide mu roller ennyogovu ennyo ejja kuba agglomerated, kyangu okuleeta okusaasaana okubi, kale ebbugumu lya roller erya 50 °C lisaanidde. Reinforcing filler esobola okuteekebwa mu bungi obutono omu ku omu, ate softener osobola okugiteeka mu kiseera kye kimu ne soft filler. Adhesion ye rubber nnene nnyo, ssaako stearate omutono, effect esingako.
Okukomya okusala n’okuyiringisiza nga ekijjuza tekinnatuuka ku kutabula mu bujjuvu kye kivaako okusaasaana obubi. Ebbugumu eringi ery’okutabula liyinza okuvaako emizingo okukwatagana, okusaasaana kwa butto mu ngeri etali ya bwenkanya n’okutuuka n’okwokya.
( II ) Okutabula kw’omutabula gwa Banbury
Chloroprene rubber olw’okutabula ebbugumu, kale obusobozi bwayo bulina okukendeezebwako katono. Okutwalira awamu ensonga y’okutikka eteekebwa ku bitundu 60%.
(1)Obudde bw’okutabula omutabula okutwalira awamu buba wakati w’eddakiika 5 ne 15. Okusobola okukola okusaasaana okulungi. Obudde bw’okutabula bwetaaga okuba obuwanvuko katono, mu kukola n’okulongoosa kwennyini, okutabula kapiira ka chloroprene, kuyinza okwawulwamu enkola zino wammanga ebbiri. (1) okutabula kapiira ak’omutindo ogwa waggulu, olw’ebipiira ebingi, naye era kyetaagisa okusaasaana okulungi, kale okutabula kulina okuba nga kwe kutabula ekyuma ekiggulawo, okujjuza okugattibwako mpolampola.
(2) okutabula kapiira ak’omutindo ogwa wansi, oba rotor y’omulongoosa n’ekisenge ky’ekisenge ky’ekituli kinene, osobola okuteeka filler nnyingi mu kiseera kye kimu.
Ebifo eby’okutabulamu omutabula wa Banbury birina ensonga bbiri:
Ekimu kwe kufumba ekintu kya kapiira ekitabuddwamu ne kifuuka omupiira;
Ekyokubiri kwe kukozesa obulungi okusala, ne kiba nti kisaasaanye bulungi.
Singa omulimu gw’omutabula banbury guba mulungi, guyinza okuba nga gufumbiddwa bulungi kapiira, osobola okulowooza ku kizibu ky’okusaasaana okulungi kwokka. Singa rotor y’omulongoosa n’ekisenge ky’ekisenge ky’ekituli biba binene, oba okutabula enkola ya kapiira entono, olwo okukamula kapiira kye kifo ekisooka, okusaasaana obulungi kye kifo ekyokubiri. Mu kiseera kino, ensonga y'okutikka erina okwongerwako okutuuka ku 65 ~ 70%, ate nga ekijjuza kiyinza okugattibwako okutwala enkola efaananako n'enkola ya 'reverse mixing'. Kwe kugamba, oluvannyuma lw’okugattako kapiira ka chloroprene, magnesium oxide, antioxidant, kitundu kya filler zonna mu kiseera kye kimu. Singa kapiira kasumuluddwa nga tosobola kunyigirizibwa mu mupiira, osobola n’okussaamu ekitundu ky’amafuta n’ebirala. Mu bufunze, tulina okugezaako okufuula kapiira akanywezeddwa mu mupiira.
Kinajjukirwa nti magnesium oxide bw’ogattibwa yokka, atera okukuŋŋaanyizibwa n’okunywerera singa ekiwujjo kiba kinnyogoga. Singa softener ne filler biteekebwamu mu kiseera kye kimu, nakyo kyangu okugatta. Teekamu amafuta ng’omaze okusaasaanya ekijjuza, oba ssaako ekijjulo ng’omaze okusaasaanya amafuta, ekikolwa ky’okusaasaanya kirungi. Okugatta ku ekyo, bw’oba okozesa kaboni omuddugavu ng’alina omuwendo omunene ogw’okunyiga amafuta, kirungi okuleka kaboni omuddugavu okusooka okunyiga amafuta nga tonnaba kugateeka mu kapiira. Mu mbeera y’okukamula obulungi kapiira mu kibinja, ekigonza kye kisembayo okuteekebwamu, olwo okusaasaana ne kuba kulungi, era kuyinza okukendeeza ku bbugumu lya kapiira. Bw’oba otabula ne banbury mixer, okusobola okuziyiza okukola carbon black gel oba okuyokya, olina okugezaako okukozesa okutabula okw’ebbugumu eritono. Naye okujjako ebbumba, calcium carbonate n’ebintu ebirala ebijjuza ebitali biramu, olw’obunnyogovu bwakyo buba bungi, ekivaamu okusaasaana obubi, singa ebbugumu lya kapiira lyeyongera okutuuka ku 100 °C okutabula, okukendeeza ku mazzi, okusaasaana kuba kulungi. Teekamu zinc oxide, accelerator mu refiner, ekifuga ebbugumu ly’okufulumya mu 105 a 110 °C, so si mu refiner nga oyongeddeko, ebbugumu ly’okufulumya lirina okuba wansi wa 125 °C. Zinc oxide ne accelerator bisinga kugattibwako mu ngeri ya maama alongoosa kapiira. Gye buvuddeko, olw’embiro za rotor y’ekyuma ekisaanuusa ebadde eyanguwa, chloroprene rubber mwangu okwokya, okutwalira awamu atera okutwala mu kusaanuusa mu bbanga ettono okutabula, okufuluma amangu, mu kuggulawo ekyuma ekisaanuusa okugattako zinc oxide, n’oluvannyuma n’okunyiga n’ebirala mu kutabula okw’emitendera ebiri Enkola y’okutabula ey’emitendera ebiri ey’okulongoosa okw’okwongerako.