Zinc Oxide-ZnO

Zinc oxide is an inorganic substance with the chemical formula ZnO, an oxide of zinc. It is insoluble in water and soluble in acids and strong bases. Zinc oxide is a common chemical additive and is widely used in synthetic rubber.
Availability:
Quantity:

Zinc oxide is an chemical compound with the formula ZnO. It is practically insoluble in water and soluble in both acids and strong bases. Zinc oxide is a major inorganic additive used widely in synthetic rubber production. ZnO is applied to the production of either natural/Synthetic rubber & latex in the Rubber or Cable Industries. It is used in these applications as a vulcanizing active agent, reinforcing agent as well as a coloring agent to allow the rubber to possess corrosive resistance, tear resistance & elasticity. It is also used as a coloring agent and filler for White Rubber, as a vulcanizing agent for Neoprene Rubber, and as a light stabilizer for fine-polded particle Plastics such as polyolefins or PVC. Herchy Rubber offers a wide range of choice of zinc oxide grades to meet different needsZinc oxide-ZnO


Zinc oxide is an inorganic substance with the chemical formula ZnO, an oxide of zinc. It is insoluble in water and soluble in acids and strong bases. Zinc oxide is a common chemical additive and is widely used in synthetic rubber.


ZnO is used as vulcanizing active agent, reinforcing agent and coloring agent of natural rubber, synthetic rubber and latex in rubber or cable industry industry to make rubber have good corrosion resistance, tear resistance and elasticity. It is used as coloring agent and filler of white rubber, vulcanizing agent in neoprene rubber and light stabilizer of plastics such as polyolefin or polyvinyl chloride for fine particles (about 0.1μm in size).


Herchy Rubber has a wide range of zinc oxide grades to choose for a variety of different needs



HerchyZnic oxide ContentActive Znic oxide ContentPb2+ ContentCu2+ ContentMn2+ ContentSpecific surface areadensityPHSieve residue(45μm)Application
gradewt%wt%wt%wt%wt%m2/gg/cm3
%
NC105min.54min.93max.0.001max. 0.0005max.0.00120-303.6

Tires, inner Tubes, Rollers, Conveyor belts, Auto parts, Soles
NC205min.50min.93max.0.001max. 0.0005max.0.001253.4

Car tires, Motorcycle Tires, Shoes, Rollers, Conveyor belts, Auto parts, Rubber profiles
NC232min.25min.25max.0.001max.0.001max.0.001


max.0.2Bicycle tires, Car parts, Rubber rings, Soles
NC23437-43
max.0.001max.0.001max.0.001

8.5-10.5max.0.5Tires, inner Tubes, Rollers, Conveyor belts, Auto parts, Soles
RAmin.40
max.0.002max.0.001max.0.00115


Shoe sole, Bicycle inner tube, Bicycle tire, Truck inner tube, Rubber parts, Rubber ball
NC23660-65min.90max.0.001max. 0.0005max.0.001403.6

Tires, inner Tubes, Rollers, Conveyor belts, Auto parts, Soles
TR80988-93
max.0.001max. 0.0005max.0.001404.6

Tires, inner Tubes, Rollers, Conveyor belts, Auto parts, Soles


1.  Tires

Improve the thermal conductivity, wear resistance, tear resistance, tensile strength and other indicators of the product, and can save about 30% of the amount of zinc oxide.


2. Rubber products

①Activated zinc oxide is mainly used as reinforcing agent of rubber to make rubber have good corrosion resistance, tear resistance and elasticity and elongation.

②It is used as accelerator of rubber vulcanization process and is multifunctional rubber compounding agent, mainly used as vulcanization active agent and reinforcing agent of natural rubber, synthetic rubber and latex.

③As vulcanization active agent, it is evenly distributed in the rubber material, has a large contact area with hydrogen sulfide, and has a greater opportunity to carry out interfacial reaction, plus the active zinc oxide products have the help of active substances to catalyze the conversion of zinc oxide into zinc sulfide.

④As a sulfide oxidizer, its function is to enhance the activity of accelerator, reduce the dosage of accelerator and shorten the vulcanization cycle.

⑤It can speed up the vulcanization speed, improve the thermal conductivity of vulcanized rubber, and make the vulcanization more complete.

⑥In the rubber industry, especially in the production of transparent rubber products, active zinc oxide is an excellent vulcanizing active agent.


3. Synthetic rubber

It is used as activator, vulcanization accelerator and reinforcing agent, and has coloring effect. Promote the vulcanization of rubber, activation and reinforcement, anti-aging effect, can strengthen the vulcanization process, improve the tear resistance and wear resistance of rubber products.


Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.