Otu ngwaahịa

Rubbers sịntetik: Njirimara zuru oke, uru na ngwa

1. Fluororubber (FKM)

  • Njirimara:

    • Nnukwu nguzogide okpomọkụ (-20°C ruo +250°C).

    • Nguzogide pụrụiche megide mmanụ, mmanụ ọkụ, ihe mgbaze, acids na ntọala.

    • Ike tensile dị elu, ntọala mkpakọ dị ala, yana nkwụsi ike kemịkalụ mara mma.

    • Ọkụ na-eguzogide ọkụ na ozone na-eguzogide.

  • Uru:

    • Na-eguzogide kemịkalụ ike na gburugburu oke nrụgide.

    • Ogologo ndụ ọrụ na ikuku ikuku na ngwa ụgbọ ala.

  • Ngwa:

    • Usoro mmanụ ụgbọ elu, O-mgbanaka, na gaskets.

    • Akara nnyefe akpaaka, hoses engine, na akụrụngwa turbocharger.

    • Kemịkalụ nhazi akụrụngwa lining na gaskets.

2. Chloroprene roba (CR)

  • Njirimara:

    • Nguzogide mmanụ na-agafeghị oke (dị mma karịa rọba eke mana ọ na-erughị FKM).

    • Ọkụ na-egbochi ọkụ nwere ihe na-emenyụ onwe ya.

    • Ezigbo nguzogide ihu igwe (UV, ozone, na mmiri).

    • Na-agbanwe agbanwe na obere okpomọkụ (-40°C ruo +120°C).

  • Uru:

    • Ọnụ-irè na mfe nhazi (extrusion / ịkpụzi).

    • Ike igwe dị elu na mgbochi abrasion.

  • Ngwa:

    • Suut mmiri mmiri, uwe aka, na ụdọ ụlọ ọrụ mmepụta ihe.

    • Adhesives maka akpụkpọ ụkwụ na ihe owuwu.

    • Jaketị eriri na mkpuchi elu ụlọ.

3. Rba Nitrile Hydrogenated (HNBR)

  • Njirimara:

    • Enwetara nguzogide okpomọkụ (ruo +150 Celsius) ma e jiri ya tụnyere NBR.

    • Iguzogide mmanu mmanu, mmiri mmiri hydraulic, na amines.

    • Ike ike dị elu na ike ọgwụgwụ.

    • Obere permeability na gas.

  • Uru:

    • Na-ejigide elasticity n'okpuru mkpughe ogologo oge na kemịkalụ siri ike.

    • Ogologo ndụ dị ogologo karịa NBR n'ọnọdụ dị oke egwu.

  • Ngwa:

    • Ngwá ọrụ na-egwupụta mmanụ na gas (packers, seals).

    • Akara oge ụgbọ ala, ihe ntụtụ mmanụ ọkụ, na akara turbocharger.

    • Ụlọ ọrụ hydraulic cylinders.

4. rọba silicone (VMQ)

  • Njirimara:

    • Okpomọkụ dị obosara (-60°C ruo +200°C).

    • Ọkpụkpụ dị elu (ruo 1000% elongation).

    • Ezigbo mkpuchi eletrik na nkwụsi ike thermal.

    • Biocompatible na inert.

  • Uru:

    • Na-ejigide mgbanwe na gburugburu cryogenic na oke okpomọkụ.

    • Na-eguzogide UV, ozone, na ihu igwe.

  • Ngwa:

    • Ngwa ahụike (catheters, implants).

    • Ngwa eletrọnịkị (insulators, igodo).

    • gaskets okpomọkụ dị elu maka oven na injin.

5. Fluorosilicon roba (FVMQ)

  • Njirimara:

    • Na-agwakọta mgbochi kemịkalụ FKM na mgbanwe VMQ.

    • Okpomọkụ dị nso: -50°C ruo +230°C.

    • Na-eguzogide mmanụ ọkụ, lubricants, na mmiri mmiri hydraulic.

    • Ntọala mkpakọ dị ala na nkwụsi ike dị mma.

  • Uru:

    • Na-eme ma na oke okpomọkụ na obere okpomọkụ.

    • Na-eguzogide ọzịza na mmanụ ụgbọ elu.

  • Ngwa:

    • Ihe mejupụtara sistemu mmanụ ụgbọ elu (valvụ, akara).

    • gaskets na njikọ njikọ dị n'oké osimiri submersible.

    • Ihe mmetụta ụgbọ ala na sistemụ njikwa ikuku.

6. Ethylene Propylene Diene Monomer (EPDM)

  • Njirimara:

    • Ozone pụtara ìhè na nguzogide ihu igwe.

    • Ike dielectric dị elu na nguzogide mmiri.

    • Okpomọkụ dị nso: -50°C ruo +150°C.

    • Obere gas permeability.

  • Uru:

    • Kacha dị ọnụ ahịa maka ngwa n'èzí.

    • Mmanya ịma jijiji na mbelata mkpọtụ.

  • Ngwa:

    • Ihu igwe ụgbọ ala, ọkpọkọ radiator, na mkpuchi ikuku.

    • Ihe mkpuchi mkpuchi ụlọ na ọdọ mmiri.

    • Igwe mkpuchi ọkụ eletrik na eriri nnyefe ike.


Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nwebiisinka     2023 Shanghai Herchy Rubber Co., Ltd. map saịtị |   Amụma nzuzo | Nkwado Site Leadong.