ʻO GA-60X1F Ka Puma Silikino Kūʻokoʻa Kūleʻa Loa (300℃)(HCR)
ʻO GA-60X1F Ultra Heat-resistant Silicone Rubber ((300 ℃) (HCR)
No ka hoʻohana ʻana: kūpono no ka hana ʻana i nā ʻāpana kaʻa, nā moena pale wela, nā sila pale wela a me nā huahana ʻē aʻe.
ʻO nā hiʻohiʻona nui: maikaʻi ka wela wela a me ka ikaika mechanical, hele i ka hōʻoia o RoHS, REACH, a me FDA.