Tare da shekaru na gwaninta a cikin samar
da roba roba ,
Herchy iya samar da fadi da kewayon
roba roba roba .
roba roba iya saduwa da yawa aikace-aikace, idan kana bukatar, don Allah samun mu online dace sabis game da
roba roba . Baya ga jerin samfuran da ke ƙasa, zaku iya keɓance na musamman
roba roba gwargwadon buƙatun ku.
Bayyanawa da yanayin: fari (m ko mai bayyanawa) toshe
Nau'in monomer na uku da abun ciki: ENB, 5.0%
abun ciki na Ethylene: 64%
abun ciki na mai: 75%
dankon Mooney: ML (1 + 4) 125 ° C 55
Girman: 25kg / toshe
MOQ: 25kg
Packing: 25kg Packing
Bayyanawa da yanayin: fari (m ko mai bayyanawa) toshe
Nau'in monomer na uku da abun ciki: ENB, 1.0%
Ethylene abun ciki: 66%
Mooney danko: ML (1 + 4) 125 ° C 46
Girman: 25kg / toshe
MOQ: 25kg
Packing: akwati
Bayyanawa da yanayin: fari (mai bayyana ko m) toshe
Nau'in monomer na uku da abun ciki: ENB, 4.1%
Ethylene abun ciki: 53%
Mooney danko: ML (1 + 4) 125 ° C 30
Girman: 25kg / toshe
MOQ: 25kg
Packing: akwati
Bayyanawa da yanayin: fari (m ko mai bayyanawa) toshe
Nau'in monomer na uku da abun ciki: ENB, 6.5%
abun ciki na Ethylene: 68%
dankowar Mooney: ML (1 + 4) 125 ° C 135
Girman: 25kg / toshe
MOQ: 25kg
Packing: akwati
Bayyanawa da yanayin: fari (mai bayyana ko m) toshe
Nau'in monomer na uku da abun ciki: ENB, 4.5%
abun ciki na Ethylene: 69%
dankowar Mooney: ML (1 + 4) 125 ° C 63
Girman: 25kg / toshe
MOQ: 25kg
Packing: akwati
Bayyanawa da yanayin: fari (mai bayyana ko m) toshe
Nau'in monomer na uku da abun ciki: ENB, 5.5%
abun ciki na Ethylene: 68%
dankowar Mooney: ML (1 + 4) 125 ° C 87
Girman: 25kg / toshe
MOQ: 25kg
Packing: akwati