Sintetiki Lastikuw , bɛɛ haminanko kɛrɛnkɛrɛnnen tɛ kelen ye a ko la, wa an bɛ min kɛ, o ye ka kiliyan kelen-kelen bɛɛ ka fɛn dilannenw magoɲɛfɛnw caya, o la, an ka
Sintetiki Lastikuw ka ɲumanya diyara kosɛbɛ kiliyan caman fɛ, wa a tɔgɔ ɲuman bɔra jamana caman na.
Herchy Synthetic Rubber have characteristic design & practical performance & competitive price, ni aw b’a fɛ ka kunnafoni wɛrɛw sɔrɔ
Synthetic Rubber kan , aw bɛ se ka anw sɔrɔ.
A cogoya ni a cogoya: finman (a jɛlen don walima a bɛ yeelen bɔ) bloki
Monomɛri suguya sabanan ni a kɔnɔfɛnw: ENB, 4,1%
Etilɛni hakɛ: 53%
Mooney sɔgɔsɔgɔninjɛ: ML(1+4)125°C 30
Bonya: 25kg/blok
MOQ: 25kg
Pake: kɛsu kɔnɔ
A cogoya ni a cogoya : finman (a jɛlen walima a bɛ yeelen bɔ) bloki
Monomɛri suguya sabanan ni a kɔnɔfɛnw: ENB, 2,3%
Etilɛni hakɛ: 57%
Mooney sɔgɔsɔgɔninjɛ: ML(1+4)125°C 35
Bonya: 25kg/blok
MOQ: 25kg