A cogoya ni a cogoya: finman (a jɛlen don walima a bɛ yeelen bɔ) bloki
Monomɛri suguya sabanan ni a kɔnɔfɛnw: ENB, 1,0%
Etilɛni hakɛ: 66%
Mooney sɔgɔsɔgɔninjɛ: ML(1+4)125°C 46
Bonya: 25kg/blok
MOQ: 25kg
Pake: kɛsu kɔnɔ
A cogoya ni a cogoya: finman (a jɛlen don walima a bɛ yeelen bɔ) bloki
Monomɛri suguya sabanan ni a kɔnɔfɛnw: ENB, 4,1%
Etilɛni hakɛ: 53%
Mooney sɔgɔsɔgɔninjɛ: ML(1+4)125°C 30
Bonya: 25kg/blok
MOQ: 25kg
Pake: kɛsu kɔnɔ