Te ahua me te ahua: ma (maamaa, maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 5.7%
Ethylene ihirangi: 58%
Mooney viscosity: ML(1+4)125°C 84
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: ma (maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 4.5%
Ethylene ihirangi: 69%
Mooney viscosity: ML(1+4)125°C 63
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: ma (maamaa, maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 1.0%
Ethylene ihirangi: 66%
Mooney viscosity: ML(1+4)125°C 46
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: ma (maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 9.4%
Ethylene ihirangi: 55%
Mooney viscosity: ML(1+4)125°C 29
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: ma (maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 5.0%
Ethylene content: 64%
Te hinu hinu: 75%
Mooney viscosity: ML(1+4)125°C 55
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: ma (maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 4.1%
Ethylene ihirangi: 53%
Mooney viscosity: ML(1+4)125°C 30
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka